Description of casting defects of cast steel joints

The description and general impression of casting defects of various cast steel joints are as follows: (1) The four cast steel joints showed the same casting defect characteristics, that is, cracks were found in R zone. These four joints are cast steel joints of gymnasium, and they are all...

spacer
spacer
spacer

NDT for casting defects of cast steel joints

According to the summary, a total of 50 casting defects were found in 24 cast steel joints, and the average number of casting defects per cast steel joint was 2.04. Among the 50 casting defects, there were 12 crack defects, accounting for 24% of all casting defects, 8 inclusion...