1 Casting porosity (1) Features and inspection methods: After dissection, appearance inspection or flaw detection showed that the pores had smooth surface and round shape. (2) Causes: ① The introduction direction of the alloy liquid is unreasonable or the flow speed of the metal liquid is too high, resulting...