Sand box and mold plate for sand casting

Casting sand box When making sand mold, we need to use a frame without bottom, cover and around the sand mold to prevent the real-time outward extrusion of molding sand. This kind of frame is called sand box. The role of the sand box is to facilitate the molding,...