The proportion of raw materials for smelting is scrap: recycled material = 4:6, and the composition of molten iron after spheroidizing treatment. The pouring temperature is 1493 ℃, the actual pouring time is 8.5 s, the pouring temperature of the first mold is 1417 ℃, and the pouring temperature...
Aug122020