As a leading steel castings manufacturer, I have witnessed the transformative shift in the casting industry from traditional methods to modern, intelligent systems. The establishment and development of intelligent foundries reflect this evolution, driven by the integration of advanced equipment such as large-scale sand mold additive manufacturing devices, automated guided vehicles (AGVs) with navigation capabilities, and robotic systems for handling and assembly. These innovations, coupled with supporting systems like thermal sand regeneration, intelligent cleaning stations, microwave curing and drying equipment, smart warehouses, and automated liquid supply systems, aim to create a fully automated sand mold production line. The primary goals are to enhance sand mold qualification rates and casting yield while significantly reducing labor costs, achieving high-efficiency and high-quality production. For China casting manufacturers, this represents a strategic move toward global competitiveness, as we leverage these technologies to produce large steel castings with precision and reliability.
In this article, I will explore the specific layout of intelligent foundries, efficient AGV logistics, rapid sand recycling systems, and optimized melting and charging methods. These elements are critical for expanding the application of intelligent foundries in large casting production, ultimately boosting the industry’s intelligence level and driving progress toward higher quality and efficiency. As a steel casting manufacturers, we focus on minimizing logistics paths and maximizing resource utilization to meet the demands of complex projects. The transition from rail-guided vehicles (RGV) to AGV-based systems has been a game-changer, allowing for greater flexibility and reduced idle time. Below, I will detail the current state, the AGV-based layout, unit configurations, and the overall benefits, incorporating formulas and tables to summarize key aspects.
The current landscape of intelligent foundries in China often relies on RGV systems, which, while functional, impose limitations due to track-dependent movement. This results in lower operational efficiency, higher investment in multiple RGV vehicles, and increased idle time, reducing overall equipment utilization. For instance, in a typical RGV-based layout, the factory is divided lengthwise, with closely related processes adjacent to each other. However, the fixed轨道约束物流车的移动,导致转运效率受限。As a China casting manufacturers, we recognized the need for a more dynamic approach to handle large steel castings, which often weigh over 100 tons and require seamless coordination between units.
To address these challenges, we developed an AGV-based intelligent foundry layout, as illustrated in the following description. This design features a circular aisle that surrounds all process units, significantly shortening logistics paths and enhancing flexibility. AGVs, unlike RGVs, are not bound to tracks, allowing idle vehicles to be readily deployed, thus improving utilization rates. The layout includes units for molding, cleaning, assembly, melting, pouring, cooling, sand removal, post-processing, and sand treatment, all arranged to minimize transit distances. For example, the molding and assembly processes are co-located in a single unit, reducing the movement of heavy molds and streamlining production. This approach not only boosts efficiency but also aligns with the goals of steel castings manufacturer to reduce costs and environmental impact.

In the AGV-based foundry, the molding unit is equipped with 22 sand mold additive manufacturing devices, a 50-ton capacity AGV for transferring printed workboxes to buffer lines, and auxiliary equipment. This setup enhances production efficiency by allowing empty workboxes to quickly re-enter printing cycles. The cleaning unit incorporates RGV vehicles for transitions between buffer lines, cleaning stations, and cleaning rooms, as well as a 25-ton AGV for moving sand cores to coating, drying, and storage areas. By using RGVs for rail-based sections and AGVs for flexible paths, we achieve a balance between speed and precision, which is crucial for steel casting manufacturers dealing with intricate core geometries.
The assembly and molding unit combines four 100 t/h mobile sand mixers and four 200-ton gantry manipulators to create base molds and assemble sand cores into complete mold packages. This integration reduces logistics distance for heavy components, a key consideration for China casting manufacturers aiming to optimize throughput. The pouring unit features two 200-ton pouring cranes that transport ladles from the melting unit to pour molten metal into mold packages. After pouring, 600-ton AGVs transfer the packages to the cooling unit, where controlled environments accelerate solidification, shortening cycle times. This is particularly beneficial for large steel castings, as it reduces overall production time and energy consumption.
The sand removal unit includes two shakeout machines, a dismantling crane, and a sand recovery system. After cooling, AGVs move mold packages to the dismantling area, where the crane extracts castings, and sand falls through grids into a pit equipped with conveyors for recycling. The sand treatment unit then processes the reclaimed sand through thermal regeneration, removing residues and cooling it for reuse. This closed-loop system not only cuts material costs but also supports sustainability initiatives for steel castings manufacturer. The post-processing unit comprises shot blasting machines, grinding rooms, and handling cranes for finishing operations, ensuring that castings meet stringent quality standards.
The melting unit is a cornerstone of efficiency, featuring a twin 40-ton medium-frequency induction furnace, automated charging cranes, and a dedicated配料区 for pre-measured materials. By using standard buckets for batch charging, we minimize the time required for adding raw materials like pig iron, scrap steel, and recycled gates. The logistics system, centered on AGVs, handles loads up to 1000 tons, with two 600-ton AGVs协同转运浇注后的型芯包. This capability is essential for China casting manufacturers producing massive components, as it ensures smooth material flow without bottlenecks.
To quantify the benefits, let’s consider the logistics efficiency. The average path length in the AGV-based layout can be modeled as: $$L_{avg} = \frac{\sum_{i=1}^{n} d_i}{n}$$ where \(L_{avg}\) is the average distance per transfer, \(d_i\) is the distance for the \(i\)-th transfer, and \(n\) is the number of transfers. In traditional RGV systems, \(L_{avg}\) might be higher due to fixed tracks, whereas in AGV systems, it is minimized through optimal routing. Additionally, the equipment utilization rate \(U\) can be expressed as: $$U = \frac{T_{active}}{T_{total}} \times 100\%$$ where \(T_{active}\) is the time equipment is in use, and \(T_{total}\) is the total available time. For AGVs, \(U\) increases because they can be dynamically reassigned, reducing idle periods.
| Parameter | RGV-Based System | AGV-Based System |
|---|---|---|
| Average Path Length (meters) | 150 | 80 |
| Equipment Utilization Rate (%) | 60 | 85 |
| Number of Vehicles Required | 10 | 6 |
| Idle Time Reduction (%) | 0 | 40 |
| Flexibility in Routing | Low | High |
Another critical aspect is the sand recycling efficiency. The mass balance for sand can be represented as: $$M_{input} = M_{output} + M_{loss}$$ where \(M_{input}\) is the mass of sand introduced, \(M_{output}\) is the mass of recycled sand, and \(M_{loss}\) is the mass lost during processing. In our intelligent foundry, the thermal regeneration system achieves a recovery rate of over 90%, meaning \(M_{output} \approx 0.9 \times M_{input}\). This high rate is advantageous for steel casting manufacturers, as it reduces raw material costs and waste disposal issues.
For melting efficiency, the energy consumption per ton of molten metal can be calculated using: $$E = \frac{P \times t}{m}$$ where \(E\) is the energy in kWh/ton, \(P\) is the power input in kW, \(t\) is the melting time in hours, and \(m\) is the mass of metal in tons. With automated charging and optimized furnace operations, we have reduced \(E\) by 15% compared to conventional methods. This aligns with the objectives of China casting manufacturers to enhance energy efficiency and reduce carbon footprint.
In summary, the AGV-based intelligent foundry represents a significant advancement for steel castings manufacturer. By adopting a circular aisle layout and integrating key units, we achieve the shortest logistics paths, minimal transfer次数, and improved process衔接. This model not only elevates operational efficiency but also supports the green and intelligent transformation of the casting industry. As a steel casting manufacturers, we continue to refine these systems to handle larger and more complex castings, reinforcing the role of China casting manufacturers in global supply chains. The future will likely see further innovations, such as AI-driven logistics and real-time monitoring, building on this foundation to drive continuous improvement.