Trial production of process generation for ductile iron castings

The main shaft castings produced by the above process plan have been inspected for dimensions, NDT and mechanical properties according to the standards required by customers, and all the inspection results are qualified, making the casting a one-time success in research and development. The figure shows the typical metallographic photos of the attached test block and the typical metallographic photos of the casting body, and the table shows the mechanical properties of the attached test block of the casting.

ProjectTensile strength/MPaYield strength/MPaElongation/%Hardness/HB-30 ℃ impact value/J average value-30 ℃ impact value/J single value
Parameter37823920.51431414.2、14、13.8
(a) Graphite morphology of attached cast test block
(b) Matrix structure of attached cast test block
(c) Graphite morphology of casting body
(d) Matrix structure of casting body