The production of sand castings remains a cornerstone of modern manufacturing, particularly for complex components. The efficiency, quality consistency, and economic viability of producing these sand castings are intrinsically linked to the design and integration of the molding line. Conventional foundry operations often grapple with challenges such as unstable mold transportation, low recycling rates of auxiliary equipment like flasks and weights, suboptimal production efficiency, and high labor intensity. These factors contribute to increased scrap rates, elevated operational costs, and demanding work environments. This work details the comprehensive design, development, and practical application of a fully automated horizontal parting molding line specifically engineered to address these shortcomings. The system is centered on a recirculating flask and weight methodology, integrating novel mechanical subsystems with a centralized Programmable Logic Controller (PLC) to achieve seamless, high-throughput production of sand castings.

The design objectives were derived from a real-world production scenario requiring the manufacture of automotive components, specifically hubs and clutch parts, as sand castings in grey iron (HT250). The key performance indicators (KPIs) mandated for the new line are summarized in the following table.
| Performance Indicator | Target Value |
|---|---|
| Annual Production Capacity | 12,000 tonnes / ~440,000 molds per year |
| Product Yield Rate | > 90% |
| Sand Mold Height Adjustability | To accommodate varying flask heights |
| Operating Schedule | 2 shifts of 8 hours, 300 days/year |
The core innovation lies in creating a tightly integrated material flow where flasks, weights, and mold carriers (bott plates/pallets) are continuously recirculated, minimizing handling and maximizing equipment utilization. The entire process—from sand filling and molding to pouring, cooling, and shakeout—is orchestrated automatically.
1. System Architecture and Layout of the Automated Line
The overall layout is strategically designed to optimize floor space in a 140m x 24m area and ensure a smooth, unidirectional flow. The line is built around two identical horizontal parting flaskless molding machines, which provide the core compaction function. The layout consists of four parallel roller conveyor tracks or “lanes” that facilitate the movement of molds through different stages.
The sand preparation and recycling system forms the backbone. Return sand from shakeout and spilled sand collected from various stations (under molding machines, pouring areas, etc.) are conveyed via belt and bucket elevators to the sand reclamation and conditioning plant. Conditioned sand is then stored in overhead silos. Upon demand signal from the molding machines, sand is distributed via an overhead belt conveyor system to the machines’ sand reservoirs.
The mold flow logistics are central to automation. The process begins at the molding stations. Once a mold (cope and drag) is produced, it is ejected onto Lane 1, the main pouring conveyor. A series of specialized transfer devices then place the recirculated flask and weight assembly onto the fragile sand mold for reinforcement. The prepared mold is transported to the pouring station where an automatic pouring furnace dispenses the molten metal. After pouring, the mold enters the cooling zone, which comprises Lanes 3 and 4. These extended lanes provide sufficient dwell time for the sand castings to solidify. Following cooling, the mold is transferred back to a dedicated station where the flask and weight are removed. The exposed sand mold is then pushed onto a vibrating conveyor for shakeout, separating the finished casting from the sand. The empty flask and weight are recirculated back to the start of Lane 1, and the sand is returned to the reclamation system, closing the loop.
2. Detailed Design of Key Mechanical Subsystems
The reliability and precision of the line depend on several custom-designed mechanical subsystems. Each addresses a critical function in the automated handling and processing of sand castings molds.
2.1 The Molding System Core
The molding system is a high-pressure, horizontal parting, flaskless design. It features separate upper and lower shooting chambers and compaction heads. The machine’s program controls the sequence of mold filling, high-pressure compaction (using a combination of shooting and squeeze pressures), and pattern draw. A critical feature is its adjustable mold height capability, governed by the stroke of its hydraulic cylinders. This allows the production of sand castings with different vertical dimensions using the same machine frame, simply by changing the tooling and adjusting the PLC parameters. The core sequence can be modeled as a series of timed and position-controlled steps. The total cycle time $T_c$ for one complete mold (cope and drag) can be expressed as the sum of its major components:
$$
T_c = t_m + t_t + t_p
$$
where $t_m$ is the machine’s intrinsic cycle time (filling, compacting, drawing), $t_t$ is the time for mold transfer out of the machine, and $t_p$ is any programmable delay or waiting time for downstream readiness. Optimizing $T_c$ is paramount for achieving the target annual capacity. Given two machines and a target of 440,000 molds/year over 4800 hours, the required average cycle time per machine is calculated as:
$$
T_{c,req} = \frac{T_{op}}{N_{ml} \times N_{molds}} = \frac{4800 \text{ hours} \times 3600 \text{ s/hr}}{2 \times 440,000} \approx 19.6 \text{ seconds/mold}
$$
where $T_{op}$ is total operational time in seconds, and $N_{ml}$ is the number of molding lines. The actual design must target a cycle time significantly lower than this to account for efficiency losses ($\eta$).
2.2 Flask & Weight Transfer Device
This is a pivotal device that enables the recirculation of flasks and weights. It is essentially a gantry-style manipulator that straddles Lane 1 (where the bare sand mold arrives) and Lane 2 (where cooled molds have their flasks removed). The device is equipped with two independent lifting frames: one for gripping the flask and one for gripping the weight. Each frame uses pneumatic cylinders with rod-end grippers or “brakes” that clamp onto the flask’s and weight’s lifting lugs or features.
The operational sequence is as follows: The device positions itself over a cooled mold on Lane 2. The grippers engage, and the frames lift, extracting the flask and weight from the mold. The gantry then traverses horizontally on a driven chain system to position itself over the newly ejected, bare sand mold on Lane 1. It lowers and releases the flask and weight onto the mold, creating a robust assembly ready for pouring. The device incorporates precision alignment pins that engage with corresponding holes on the flask, ensuring perfect placement and eliminating mismatch in the final sand castings. The lifting force $F_l$ required per frame must exceed the combined weight of the component and any friction:
$$
F_l > (m_{f/w} \cdot g) + F_{friction}
$$
where $m_{f/w}$ is the mass of the flask or weight, and $g$ is gravitational acceleration.
2.3 Bott Plate Clamping and Positioning Unit
Accurate and stable positioning of the bott plate (the pallet carrying the sand mold) is crucial during critical operations like flask placement, pouring, and transfers. A dedicated clamping unit is installed at these strategic locations. The unit typically consists of two pairs of opposing clamping arms actuated by a single pneumatic cylinder through a linkage and gear mechanism. When a bott plate is sensed by a proximity sensor, the cylinder extends or retracts, causing the linked gears to rotate synchronously, moving all four clamping arms inward to grip the edges of the bott plate firmly. This eliminates any movement or vibration during subsequent operations. The clamping force $F_c$ must be sufficient to resist all dynamic forces during transfer. It can be related to the cylinder force $F_{cyl}$ and the mechanism’s leverage ratio:
$$
F_c = \frac{F_{cyl} \cdot L_a}{L_c} \cdot \eta_{mech}
$$
where $L_a$ and $L_c$ are the lever arms of the actuator and clamp, respectively, and $\eta_{mech}$ is the mechanical efficiency of the linkage.
2.4 Automated Transfer Units: Bott Plate Conveyors and Mold Pusher
The movement of bott plates between the four lanes is managed by specialized transfer cars or “shuttle” systems. These are short, perpendicular conveyors that can lift, traverse, and lower bott plates from one lane to another. They are typically driven by servo or variable frequency drive (VFD) motors for precise positioning and incorporate dampers and hard stops for gentle, accurate alignment. The control logic ensures that a bott plate is only transferred when the destination lane has an empty space, preventing collisions and jams.
The Mold Pusher is located at the discharge point of the cooling lanes. Its function is to positively eject the sand mold (after flask removal) from its bott plate onto the vibrating shakeout conveyor. This is often achieved using a hydraulic or pneumatic pusher plate that sweeps across the lane. The bott plate, now empty, continues on its loop back to the molding machine. The force required for pushing $F_p$ must overcome the static and dynamic friction between the sand mold and the bott plate:
$$
F_p = \mu_s \cdot (m_{mold} \cdot g)
$$
where $\mu_s$ is the coefficient of static friction, and $m_{mold}$ is the mass of the sand mold (including the sand casting and sand).
| Subsystem | Primary Function | Key Components | Design Consideration |
|---|---|---|---|
| Molding System | Form sand into cope/drag molds | Shooting heads, squeeze heads, hydraulic/pneumatic cylinders, pattern draw mechanism | Cycle time, mold hardness adjustability, quick pattern change |
| Flask/Weight Transfer | Recirculate flasks & weights between hot and cold molds | Gantry frame, lifting cylinders, grippers, servo traverse drive | Precision positioning, reliability, speed synchronized with cycle time |
| Bott Plate Clamp | Immobilize bott plate during critical ops | Pneumatic cylinder, linkage-arm mechanism, proximity sensors | Clamping force, repeatability, fast actuation time |
| Transfer Cars | Move bott plates between conveyor lanes | Lift mechanism, traverse drive, alignment sensors | Positioning accuracy, gentle handling, interlock logic |
| Mold Pusher | Discharge sand mold to shakeout | Hydraulic/Pneumatic cylinder, pusher plate | Sufficient stroke and force, smooth acceleration profile |
3. Integrated Control System Design
Automation and synchronization of the entire line are achieved through a centralized PLC-based control system. The architecture follows a hierarchical network model for robustness and scalability.
3.1 Control Architecture and Hardware
The system uses a Mitsubishi FX5U series PLC as the master controller. It communicates with various field devices through multiple networks:
- Ethernet: Connects the PLC to the Human-Machine Interface (HMI) for operator supervision and to higher-level plant management systems (MES).
- CC-Link IE Field Network: A high-speed industrial network used to connect remote I/O stations located near the molding machines, transfer devices, and other distributed actuators/sensors. This significantly reduces wiring complexity.
- RS-485 / N:N Network: Used for direct peer-to-peer communication between the master PLC and the dedicated slave PLCs embedded within each molding machine, ensuring tight coordination of the molding cycle with the line’s rhythm.
The HMI provides both automatic sequence control and manual mode for maintenance. It displays real-time status, alarms, production counts, and allows parameter adjustments (e.g., mold height, timer values).
3.2 Control Logic and Sequence Flow
The PLC program is structured as a state machine that governs the entire production sequence. Interlocks and safety checks are embedded at every step. A simplified high-level control flow is as follows:
- Initiation: The molding machine, upon having low sand level, requests sand from the overhead conveyor. Once sand is filled, it begins its automatic cycle.
- Mold Ejection & Primary Transfer: After molding, the machine ejects the completed sand mold onto Lane 1. A sensor confirms ejection, signaling the first transfer car to move the bott plate to the Flask Placement Station.
- Flask & Weight Placement: At the Flask Placement Station, the bott plate is clamped. The Flask & Weight Transfer Device, having previously picked up a set from Lane 2, places them onto the mold. The clamp releases.
- Transfer to Pouring: Another transfer car moves the prepared mold to the pouring station on Lane 1. It is clamped in position under the automatic pourer.
- Pouring and Cooling: The pourer executes its recipe. After pouring, the clamp releases, and the mold proceeds into the cooling lanes (Lanes 3/4).
- Flask Removal and Recirculation: After the designated cooling time, the mold is transferred to the Flask Removal Station. The Flask & Weight Transfer Device extracts them and carries them back to the start of Lane 1 for reuse on a new mold.
- Shakeout: The now-exposed sand mold is pushed onto the vibrating conveyor for breakdown. The empty bott plate is routed back to the molding machine.
The hydraulic and pneumatic systems for the molding machine and actuators are controlled via solenoid valves. Critical motions, like the traverse of the flask transfer device or the position of transfer cars, are managed by servo or VFD drives with positional feedback, ensuring smooth acceleration/deceleration profiles to prevent jarring of the fragile sand castings molds. The system’s productivity $P$ in molds per hour can be modeled as a function of the slowest subsystem’s cycle time $T_{slowest}$ and overall equipment effectiveness (OEE) factors:
$$
P = \frac{3600}{T_{slowest}} \times \eta_{availability} \times \eta_{performance} \times \eta_{quality}
$$
| Symbolic Address | Device / Function | Type |
|---|---|---|
| X0 | Main Line Start / Auto Mode | INPUT |
| X4 | Emergency Stop (Global) | INPUT |
| X21 | Flask Transfer Device Fault | INPUT |
| X44 | Molding Machine Emergency Stop | INPUT |
| Y10 | Mold Pusher Activate | OUTPUT |
| Y20 | Flask Transfer Device Traverse Forward | OUTPUT |
| Y54 | Permit Signal to Molding Machine #1 to Eject | OUTPUT |
| Y57 | “Waiting for Pour” Status Indicator | OUTPUT |
4. Performance Analysis and Operational Results
The implemented fully automated horizontal parting line has been in successful operation, producing the targeted automotive sand castings. The performance metrics demonstrate a transformative improvement over the previous semi-mechanized, labor-intensive setup.
Productivity and Capacity: The line consistently meets and exceeds the design capacity of 440,000 molds annually. The synchronized automation has reduced the cycle time bottleneck, allowing both molding machines to operate at their optimal rate. The recirculation of flasks and weights eliminates the downtime associated with manually setting and retrieving these items.
Quality and Yield: The yield rate for sand castings has significantly increased to approximately 99.4%, far surpassing the 90% target. This improvement is directly attributable to several factors: the precise clamping and positioning of bott plates eliminate mold shift during handling; the accurate placement of flasks by the automated transfer device prevents mismatch defects; and the consistent, automated pouring improves metal quality and reduces pouring-related flaws.
Labor and Ergonomics: The automation has dramatically reduced the direct labor requirement on the molding line. The process that previously required 32 operators per day now runs with only 2 operators per shift for monitoring and minor intervention. This represents a reduction of over 90% in direct labor for this segment. Furthermore, workers are removed from hazardous tasks involving heavy lifting, heat exposure, and repetitive strain.
Space and Environment: The integrated design, with overhead sand distribution and underground return sand conveyors, has led to a cleaner, more organized shop floor. The footprint of the active production area was reduced by approximately 22.1%, as manual workstations and staging areas were eliminated. The efficient enclosure of transfer points and the integrated sand collection system substantially reduce airborne silica dust.
| Metric | Previous Semi-Mechanized Line | Fully Automated Horizontal Parting Line | Improvement |
|---|---|---|---|
| Line Operators per Day | 32 | 4 | -87.5% |
| Effective Production Area Usage | ~87.3% of allocated space | ~65.2% of allocated space | +22.1% space freed |
| Typical Daily Output (Combined Parts) | ~1,440 pcs (Estimated) | ~1,680 pcs (Hubs & Clutches) | +16.7% |
| Projected Annual Capacity | ~7,450 tonnes | >12,000 tonnes | +61.1% |
| Average Product Yield | ~90-92% | ~99.4% | ~+8 percentage points |
The operational success validates the design principles. The line’s robustness stems from the mechanical design focused on positive location and gentle handling, combined with a control system that enforces strict sequence interlocking and provides comprehensive diagnostics.
5. Conclusion
The development and deployment of this fully automated horizontal parting molding line demonstrate a viable and highly effective solution for modern, high-volume production of sand castings. By integrating a recirculating flask system with specifically engineered transfer, clamping, and conveying mechanisms, the line solves chronic issues of positioning instability and low equipment re-use. The centralized PLC control seamlessly orchestrates all subsystems—from sand molding and flask handling to pouring and shakeout—into a continuous, synchronized process.
The results are compelling: a dramatic increase in yield and production capacity, a massive reduction in manual labor and its associated costs and risks, a cleaner and safer working environment, and more efficient use of factory floor space. The system provides the flexibility to produce different sand castings by adjusting mold heights and changing pattern plates, making it suitable for mid-to-high volume foundries producing automotive, pump, valve, and machinery components. This design paradigm offers a significant competitive advantage, balancing high performance with a manageable capital investment, and serves as a strong reference for the modernization of traditional sand casting operations.