In modern industrial manufacturing, sand casting remains a critical process for producing complex metal components with intricate geometries. This article presents a comprehensive analysis of mold design strategies for turbine cover castings, focusing on structural optimization, defect mitigation, and process reliability.

1. Component Structural Analysis
The turbine cover features:
- Uniform wall thickness of 4mm
- Curved volute section with 70mm downward flange
- Radial distribution of 8 mounting bosses
- Internal trumpet-shaped channel (14mm maximum thickness)
| Feature | Dimension | Tolerance |
|---|---|---|
| Wall thickness | 4±0.5mm | ASTM B85 |
| Flange height | 70±1mm | ISO 8062 |
| Boss diameter | Φ12±0.3mm | Custom |
2. Sand Casting Process Design
The feeding system follows Chvorinov’s rule for solidification control:
$$ t = B \left( \frac{V}{A} \right)^2 $$
Where:
t = Solidification time (s)
B = Mold constant (s/mm²)
V = Volume (mm³)
A = Surface area (mm²)
| Process Parameter | Value |
|---|---|
| Pouring temperature | 720±10°C |
| Cooling rate | 15-20°C/s |
| Mold hardness | 85-90 (B scale) |
3. Mold System Configuration
The sand casting mold assembly comprises:
- Pattern system with false box technology
- Composite core system (3 sand cores + 1 metal core)
- Cooling system with external chills
3.1 False Box Design
The curved parting surface requires specialized tooling:
$$ \theta = \arctan\left(\frac{\Delta h}{L}\right) $$
Where:
θ = Parting surface angle (°)
Δh = 11mm height variation
L = 150mm horizontal span
| Component | Material | Surface Finish |
|---|---|---|
| False box | GG25 cast iron | Ra 3.2μm |
| Pattern plate | AlSi7Mg | Ra 1.6μm |
3.2 Core System Design
The composite core system ensures dimensional accuracy:
| Core | Function | Material |
|---|---|---|
| Core I | Volute formation | Furan resin sand |
| Core II | Trumpet channel | Chromite sand |
| Metal core | Heat extraction | H13 tool steel |
3.3 Cooling System Design
External chills prevent shrinkage porosity:
$$ Q = k \cdot A \cdot \Delta T \cdot t $$
Where:
Q = Heat extraction (J)
k = Thermal conductivity (W/m·K)
A = Chill surface area (m²)
ΔT = Temperature differential (K)
t = Contact time (s)
4. Process Validation
Production trials confirmed:
- Dimensional accuracy: IT13-IT14
- Surface quality: Ra 12.5μm (as-cast)
- Defect rate: <0.5%
| Quality Parameter | Result | Standard |
|---|---|---|
| Pressure tightness | 5 bar/5min | ISO 11439 |
| X-ray inspection | Class B | ASTM E155 |
5. Technical Advantages
The sand casting solution demonstrates:
- Complex geometry accommodation
- Cost-effective tooling
- Flexible production scalability
| Comparison | Sand Casting | Die Casting |
|---|---|---|
| Tooling cost | $15,000 | $150,000 |
| Lead time | 4 weeks | 12 weeks |
6. Conclusion
This sand casting mold design successfully addresses the challenges of complex turbine cover production through:
- Advanced false box technology
- Optimized core system integration
- Precision thermal management
The developed solution proves sand casting remains competitive for medium-complexity components requiring tight tolerances and pressure integrity.