The molten steel of steel castings has high melting point, poor fluidity, large shrinkage and easy oxidation. Therefore, the gating system is required to be simple in structure, large in sectional area, fast and stable in filling, and have an appropriate rate of liquid level rise. An open gating system is used, as shown in the figure, and the sectional area ratio of each part meets the following requirements: