Analysis and Research on Fracture Problem of an Engine Main Bearing Cover
1. Introduction In the operation of an engine, the main bearing seat endures diverse loads. The force from the combustion […]
1. Introduction In the operation of an engine, the main bearing seat endures diverse loads. The force from the combustion […]
Abstract: This article delves into the casting process design for a large ductile iron bearing cover, addressing the common issues
Abstract This study investigates the casting process design for a large ductile iron bearing cover used in diesel engines. The