Development and present situation of casting coating
1. Casting coating theory (1) The mechanism of anti sticking sand, including sintering stripping theory, bright carbon theory and so […]
1. Casting coating theory (1) The mechanism of anti sticking sand, including sintering stripping theory, bright carbon theory and so […]
Bauxite 90%, quartz powder 10%, phenolic resin 2%, white emulsion 2%, calcium bentonite 3%, washing powder 0.1%, isopropanol 0.1%, appropriate
1.Paint composition For the preparation of magnesia powder 30-50%, pearlescent powder 20-40%, mica powder 15-30%, silica sol 3-9%, white emulsion
The strength of casting coating can not be divided into two situations: one is the normal drying strength, the other
When the dosage of HB type suspending agent is 1 phr, the suspending property has reached 97%. The surface strength