Isothermal salt bath and tempering of spheroidal graphite cast iron
In order to obtain ADI material with stable structure and performance, the salt bath used for isothermal transformation should have […]
In order to obtain ADI material with stable structure and performance, the salt bath used for isothermal transformation should have […]
Inoculation treatment: inoculation treatment of nodular cast iron can improve the roundness of graphite ball, improve the spheroidization rate, and
The common graphite forms in spheroidal graphite iron contain globular graphite type, quasi-spherical temper graphite type, interdendritic graphite type and