Precision casting, roasting and pouring technology of driving wheel
1. Roasting The average thickness of the casting shell of the driving wheel reaches 30 m, and the local thickness
1. Roasting The average thickness of the casting shell of the driving wheel reaches 30 m, and the local thickness
4.1 water glass binder is used for coating, quartz powder is used for surface layer powder, and bauxite is used
1. Determination of welding and Pouring Scheme Whether the selection of welding and pouring scheme is reasonable or not is
Operation procedure: Preparation: 1) Check the condition of furnace body: check whether the furnace lining, copper tube induction coil, cooling
Operation procedure: Check whether the baking furnace and temperature control meter are normal and whether the furnace bed is flat
Operation procedure: Before coating and hanging the surface layer, check whether the cleaned module has dropped parts, and check whether