Archives

Factors affecting the service life of tractor track shoes

1.Soil abrasive particles and medium The aggravation of wear at each wear part of tractor track shoe is closely related to the characteristics of soil abrasive particles and medium conditions. According to the measurement of energy spectrum probe, the soil is widely distributed on the wear surface, especially in...

spacer

Wear types of tractor track shoes

Because the stress state of tractor track shoe is complex and the working conditions have a great influence, the damage of tractor track shoe is the result of the comprehensive action of several different wear types. In the microscopic analysis of the worn parts of tractor track shoes, the...

spacer

Micro analysis of tractor track shoe surface wear

The micro analysis of the worn surface of tractor track shoe is of great significance to study its wear characteristics and failure mechanism, reasonably select materials and treatment technology, and improve the service life of tractor track shoe. 1.Research methods Through investigation, the severely worn tractor track shoes were...

spacer
spacer

Field wear test of tractor track shoes

In recent years, the track shoe research group has conducted 21 joint loading tests in Guangdong (paddy field), Northeast China and Henan (dry field). Based on these results, we draw the thickness dimension change of the worn part of the track shoe( Δ 50) It is a comparative block...