Analysis and Countermeasures for the Occurrence of Gas Hole and Shrinkage in Ductile Iron Tray Castings
Abstract This article delves into the structure and technical specifications of ductile iron tray castings, focusing on the issues of […]
Abstract This article delves into the structure and technical specifications of ductile iron tray castings, focusing on the issues of […]
Abstract This paper presents an analysis of the surface slag defects observed in heavy-section machine tool tray castings produced by
Abstract:This comprehensive article delves into the intricacies of gas hole and shrinking defects in large QT400-15 tray castings, which are
1. Casting Basic Information and Technical Requirements Information Details Casting Outline Size Approximately 800 mm×800 mm×200 mm Product Weight 700