The Casting Process of Part Structure

<p style=”text-align: left;”>Casting Structure:</p>
<p style=”text-align: left;”>It refers to appearance , inner cavity, wall thickness, the connection form between the wall and the wall , strengthening rib, bead of the <em><strong>casting part</strong></em>,etc.</p>
<p style=”text-align: left;”>The casting process of part structure(manufacturability of casting structure), refers to casting structure design the above-mentioned whether use the most economical method to produce ability which is complied with the design requirement.</p>
<p style=”text-align: left;”>Requirements of part structure of casting properties.</p>
<p style=”text-align: left;”>The wall thickness of the casting part should be appropriate.</p>
<p style=”text-align: left;”>If too small,will be easy to produce defects such as misrun, old septal ,etc.</p>
<p style=”text-align: left;”>If too large: coarse grain, easy to produce defects such as the contraction cavities,shrinkage porosity ,etc.</p>
<p style=”text-align: left;”><img class=”ngg-singlepic ngg-center alignleft” alt=”casting part” src=”https://www.casting-metal.com/wp-content/gallery/metal-casting/casting-part.jpg” width=”301″ height=”329″ />The Casting Shape,</p>
<p style=”text-align: left;”>Should be conducive to reducing and simplifying surface of mold parting .</p>
<p style=”text-align: left;”>The number of sub type mold surface should be as little as possible</p>
<p style=”text-align: left;”>And should avoid the uneven parting surface as far as possible;</p>
<p style=”text-align: left;”>In order to facilitate modeling.</p>
<p style=”text-align: left;”>Inclination of Structure:Inclination of the parts structure itself</p>
<p style=”text-align: left;”>Purpose:Easy to get out appearance</p>
<p style=”text-align: left;”>Wall of Internal and external shall have corresponding inclination.</p>
<p style=”text-align: left;”>The passage above talks about casting process of part structure.</p>
<p style=”text-align: left;”>This is for your reference only.</p>