Verification of simulation results of horizontal centrifugal casting of cylinder liner

As shown in the figure, it is produced with the help of computer simulation φ 400mm and φ Rough finished products of 580mm centrifugally cast cylinder liners.

It can be seen that the horizontal centrifugal casting of cylinder liner has complete mold filling and good forming quality, which verifies the accuracy of the simulation results.

Texture of materialMold temperature / ℃Molten iron weight / kgPouring temperature / ℃Pouring time / SSpeed / (R · min - 1)
CrNiCuP200±50760±31410±20100±20540±20

The final optimized process parameters are shown in Table 1 and table 2.

Texture of materialMold temperature / ℃Molten iron weight / kgPouring temperature / ℃Pouring time / SSpeed / (R · min - 1)
Vanadium titanium cast iron180±302166±31410±30240±20400±20