This paper presents a systematic approach to sand casting process optimization through the integration of CAD/CAE/CAM technologies. Focusing on a heavy-duty coupling component case study, we demonstrate how modern computational tools enhance traditional foundry practices while addressing critical challenges in sand casting quality control and production efficiency.

1. Mechanical Analysis for Casting Process Design
Fundamental equations governing stress distribution in sand casting components:
$$ \sigma_{\text{max}} = \frac{My}{I} $$
Where \( M \) = bending moment, \( y \) = distance from neutral axis, \( I \) = moment of inertia. Finite element analysis revealed critical stress concentrations in coupling flange regions:
| Location | Stress (MPa) | Safety Factor |
|---|---|---|
| Flange root | 56.96 | 2.15 |
| Bolt hole | 42.33 | 2.89 |
2. Gating System Optimization
Key parameters for sand casting gating design:
$$ Q = \frac{W}{\rho t} $$
Where \( Q \) = flow rate (cm³/s), \( W \) = casting weight (kg), \( \rho \) = metal density (g/cm³), \( t \) = filling time (s). Optimized parameters for ductile iron QT500-7:
| Parameter | Initial | Optimized |
|---|---|---|
| Pouring Temperature (°C) | 1460 | 1350 |
| Filling Time (s) | 13.4 | 15.97 |
| Riser Volume (%) | 8.4 | 10.2 |
3. Solidification Simulation
Governing equations for sand casting thermal analysis:
$$ \frac{\partial T}{\partial t} = \alpha \nabla^2 T $$
Where \( T \) = temperature, \( t \) = time, \( \alpha \) = thermal diffusivity. Simulation results showed 62% reduction in shrinkage defects through optimized cooling:
| Defect Type | Initial Probability | Final Probability |
|---|---|---|
| Macroshrinkage | 34% | 9% |
| Microporosity | 28% | 7% |
4. Tooling Design & Machining
Critical parameters for sand casting mold machining:
$$ \text{MRR} = \frac{W}{\rho t_m} $$
Where MRR = material removal rate (cm³/min), \( W \) = stock removal (kg), \( t_m \) = machining time (min). CAM programming achieved 92% toolpath efficiency with:
| Process | Tool Diameter (mm) | Feed Rate (mm/min) |
|---|---|---|
| Roughing | 40 | 1400 |
| Semi-finishing | 20 | 800 |
| Finishing | 6 | 300 |
5. Process Validation
The integrated CAD/CAE/CAM approach reduced sand casting development time by 40% while improving yield rate from 82% to 93%. Key quality metrics:
| Parameter | Traditional | Optimized |
|---|---|---|
| Dimensional Accuracy (mm) | ±1.5 | ±0.3 |
| Surface Finish (Ra) | 12.5μm | 6.3μm |
| Mechanical Properties | 85% Spec | 102% Spec |
This systematic integration of digital technologies demonstrates significant potential for advancing sand casting processes in heavy machinery manufacturing. The methodology enables precise control of complex thermal-mechanical interactions inherent in sand casting while maintaining cost-effectiveness for medium-volume production.