Effect of Normalizing Temperature on Microstructure and Mechanical Properties of G18CrMo2-6 Steel Casting
The influence of normalizing temperature (850–1000 °C) on the microstructure and mechanical properties of G18CrMo2-6 steel casting was systematically investigated.