Riser design of high carbon steel roll casting
Through the observation of the defects, it is found that the defects are shrinkage porosity and shrinkage cavity, which are […]
Through the observation of the defects, it is found that the defects are shrinkage porosity and shrinkage cavity, which are […]
Diesel engine is widely used, working environment is poor, working time is long. Because the cylinder head of diesel engine
1. Static structural analysis Finite element static structural analysis is carried out for the box type and deep cavity type
Although the metallurgical quality of molten iron is affected by many factors, foundry workers have found the quantitative index of
After the sample navigation is completed, the detection can be started, as shown in Figure 1. Move the sample table
1. Set ice pack and extend setting time appropriately Through X-ray examination and local dissection, it is found that the
As shown in Figure 1, a low-pressure casting water-cooled housing for electric bus is in the shape of a drum
The original material of zc170 cylinder head is HT300, the technical requirements are WCu = 0.5% ~ 0.8%, WCR =
After adjusting the production conditions to the appropriate level, the batch trial production was carried out, and it was found
1. Primary raw materials Q12 pig iron, industrial scrap, vermicularizing agent (wre = 9% – 11%, WMG = 4% –
1. Component classification block The structure of the valve plate of the automobile gearbox is complex and has a large
It is very important to select the appropriate carbon equivalent or carbon silicon content for the production of sound castings
In the solidification process of metal nonmetal system, nonmetal matter can be the core of metal crystallization, but metal can
Although the atomic radius of oxygen is very small (0.66), it is a highly active element and can form compounds
1. Carbon, silicon and carbon equivalent When the carbon equivalent is at the eutectic point, the casting process performance is
Among the three gas elements, the solubility of oxygen in liquid or solid cast iron is the smallest, but the
1. Defect analysis (1) The inner cavity of the cylinder body is a long strip-shaped sand core, and the gas
Nitrogen contained in cast iron mainly comes from atmosphere, various furnace charges and molds. Generally, nitrogen is not contained in
1. Defect analysis (1) The slag cleaning treatment of molten iron is not complete; (2) The results show that the
There are two forms of nitrogen in cast iron: one is dissolved nitrogen; The other is to form nitride with
1. Defect analysis (1) There is a great difference in the wall thickness between the cylinder body and the shaft
Cast heat-resistant aluminum alloy is a kind of aluminum alloy which is prepared by casting, has good oxidation resistance and
In alloy 2, the nucleation and growth of primary carbides are in the high temperature liquid phase, and there is
In China’s power industry system, many high-power units have been running for a long time, and there are deviations between
The content and spacing of eutectic structure, the content and distribution of different phases in eutectic structure of two kinds
1. Defect analysis (1) The stiffness of the base frame of the model is not enough, and the model is
The graphite content and spheroidization rate reflect the degree of graphitization and spheroidization. The typical morphology of graphite balls in
The basic structure of roller casting includes barrel and shaft head, which is in the shape of revolving body. The
The effect of semi-solid forming process is better than other methods such as modification. However, the possibility of defects (shrinkage
The figure shows the solidification cooling curve of nodular cast iron with different Nb content. It can be seen that