Casting Process Design and Production of Rod-shaped Wear-resistant Cast Iron Castings
This paper presents the casting process design and production practice of a rod-shaped wear-resistant cast iron casting. The shell molding
This paper presents the casting process design and production practice of a rod-shaped wear-resistant cast iron casting. The shell molding
As one of the important components of the balance suspension system for heavy-duty commercial vehicles, the balance axle bracket connects
1.The content of carbon, silicon, manganese, rare earth and magnesium must be appropriate. High carbon content can reduce the tendency
The characteristics of spheroidization decline: good spheroidization before furnace, poor spheroidization on castings; or good spheroidization of castings poured first
The shrinkage porosity and porosity are more common in ductile iron than in ordinary gray iron. To prevent them, more
The bad spheroidization means that the spheroidization does not achieve the expected effect. The metallographic structure of poor spheroidization is:
As the iron casting technology developing, cast iron castings are used in many place and industries. With high compressive strength,