Audio Frequency Detection Method and Device for Casting Crack Defects
1. Introduction and Research Significance In recent years, the rapid development of metallurgy, aviation, shipbuilding, architecture, and heavy machinery has
1. Introduction and Research Significance In recent years, the rapid development of metallurgy, aviation, shipbuilding, architecture, and heavy machinery has
In this work, I aimed at eliminating the severe shrinkage porosity defects that occur during the investment casting of a
In the process of manufacturing mechanical components, various defects may emerge, posing serious threats to equipment operational safety. The inspection
As a fundamental manufacturing process, sand casting remains one of the most versatile and widely adopted methods for producing metal
Surface quality control is an essential requirement in both additive manufacturing and conventional casting industries. Porosity is one of the
Cast iron, particularly gray cast iron and ductile iron, remains one of the most important engineering materials in modern manufacturing.
In this work, I present a comprehensive study on the optimization of the sand casting process for a spray pump
1. Introduction The global energy landscape is undergoing a profound transformation, shifting towards low-carbon, pollution-free, safe, affordable, and sustainable energy
In my research, I focus on the automatic detection of internal defects in sand foundry defect specimens using ultrasonic testing
Chapter 1: Introduction Sand foundry defect, particularly gas porosity, represents one of the most prevalent and technically challenging defects encountered
My research focuses on applying solidification simulation technology to improve casting production quality, with a particular emphasis on predicting and
This paper presents a comprehensive Six Sigma DMAIC approach to reduce the high rejection rate caused by sand foundry defects
In my daily work as a foundry quality engineer, I have been dealing with a persistent problem: hole-type defects in
In the production of automotive crankshafts, the occurrence of hole-type defects remains one of the most challenging quality issues. Drawing
In the modern manufacturing industry, sand foundry defect detection plays a critical role in ensuring product quality and safety. Castings
This thesis focuses on the image simulation of shrinkage cavity and porosity defects in castings, particularly within the framework of
1. Introduction to Casting Simulation and Sand Foundry Defect Control The foundry industry plays a vital role in the manufacturing
In this thesis, I present a comprehensive study on the recognition of internal defects in aerospace light-alloy castings using X-ray
In my research, I focus on the detection of sand foundry defect on industrial castings. The casting industry is one
This thesis presents a comprehensive investigation into the application of infrared thermographic nondestructive testing (NDT) for the detection of internal
As the power transmission and transformation industry continues to advance, Gas Insulated Switchgear (GIS) has become widely adopted due to
In my research, I focus on developing an automated visual inspection system for sand foundry defects. The work is motivated
The foundry industry has a long history and continues to expand its scale in modern industrial production. Casting processes are
This dissertation addresses critical manufacturing challenges encountered during the production of the CPR1000 nuclear main pump bearing support, a heavy-section
In the present work, I systematically studied the influence of coating wettability to liquid polystyrene (the decomposition product of foamed