Our cast aluminum adopts advanced tech. During the cast aluminum process, we use sand casting way and die casting way. We cast the aluminium into the slab. We also cast the aluminium into the billet. Then we can form finished or semifinished aluminum foundry. We also use lost foam casting and other casting good methods in the manufacturing process of cast aluminum.

During the cast aluminum process, we use durable and stable patterns to make the mold. The sand mold forming process is very important and critical in the cast aluminum products manufacturing. We use green sand type and dry sand type to make the mold. We can make different size and shape cast aluminum products with green sand mold and dry sand mold or both together.
We pour the melted aluminium into the cavity and fill it. We can design complicated size and shape cast aluminum mold with a mature manufacturing experience. We also adopt smaller pressure method to make the melting liquid forcefully enter into the smaller pressure area or hollow cavity to make very complicated cast aluminum products. We also adopt using big pressure method in cast aluminum manufacturing. So we can make high quality different size and shape cast aluminum products.