Prediction of several main casting defects
1) Prediction of shrinkage porosity and porosity Shrinkage cavity and shrinkage porosity are the holes that appear when the temperature
1) Prediction of shrinkage porosity and porosity Shrinkage cavity and shrinkage porosity are the holes that appear when the temperature
1. Application case carbon emission estimation The material of a casting is HT150, which is produced in batches. As shown
With the rapid development of economy, the domestic demand for large and complex parts is increasing in the fields of
1. Energy consumption of sand casting production system The carbon emission of sand casting production system is related to energy
Numerical simulation of casting filling is to analyze the heat transfer phenomenon and forming ability of high temperature liquid metal
China’s automobile industry is booming and has become the pillar industry of national economic development. However, China’s automobile industry still
1. Carbon emission source of sand casting production system A large amount of waste gas produced by sand casting production
Rapid Prototyping technology relies on the point by point accumulation forming of materials, which is not restricted by the manufacturability
The casting process of part structure usually refers to that the structure of the part itself should meet the requirements
Features: Coarse graphite: the size of graphite in the metallographic structure is very large, or there is massive graphite, and
Features: Poor lower core (core deviation, core dropping, sand squeezing and core breaking) Causes: A. Mask is not adjusted well,
When the wall thickness of high-temperature alloy castings such as adjusting piece and sealing piece is changed from 1.1mm to
Features: The white cast is hard and brittle, and it is difficult to break and turn white Causes: A. Casting
1, Characteristics There are defects in some parts of the casting, which often appear in the thin-walled part, the farthest
Fast graphite fragmentation The broken fast graphite is a kind of deformed graphite which often appears in the large end