Porosity casting defects of bucket teeth
Porosity is one of the most common casting defects in castings. According to the different formation mechanism, it is mainly […]
Porosity is one of the most common casting defects in castings. According to the different formation mechanism, it is mainly […]
Squeeze casting technology continuously applies pressure to the liquid metal in the forming process, which makes the liquid metal solidify
There is a layer of sand particles on the surface of castings that are difficult to remove, which is called
Take the bucket tooth sleeve of loader as an example (as shown in Figure 1). The single blank mass of
Shell mold casting, a casting method for producing castings with thin shell mold. A kind of molding sand (phenolic resin
Therefore, we analyze and sort out the causes of sand sticking in cast wear-resistant low alloy steel and the preventive
At present, the manufacturing processes of excavator bucket teeth in China mainly include sand casting, forging manufacturing and precision casting.
The bucket teeth on the excavator are the combination of the tooth tip and the tooth seat (see Fig. 1
Bucket teeth are the main vulnerable parts of the open pit excavator. The casting has a unit weight of 130kg,
1. Pattern making The quality of pattern is one of the keys to the success or failure of lost foam
The loading of rock (hardness f = 12-14) in a mine is mainly completed by w-1001, w401 and km-602a excavators.
With low carbon and low alloy steel zg14crmnsini, the wear resistance and hardness of bucket teeth are improved by advanced
The structure of xqc460tl-c bucket teeth studied in this paper has changed the symmetrical structure of the original bucket teeth,
At present, the forming technology of bucket teeth mainly includes sand casting, metal mold casting, lost foam casting and liquid
In recent years, researchers at home and abroad have made great achievements in the research of bucket tooth alloy materials.
Based on the use of bucket teeth in production, according to the components of bucket teeth, they can be divided
1. Improvement of structure From the actual failure of the bucket teeth, it is found that the tooth tip is
The bucket teeth need to bear the impact and bending moment from the material when contacting the material. During the
Excavator is a common important construction machinery, which is widely used in many industries of national economic construction, and plays