Sand sticking defects on the surface of wet molding clay sand steel castings
Surface sand sticking defect refers to the adhesion of a layer of sand particles on the surface of steel castings
Surface sand sticking defect refers to the adhesion of a layer of sand particles on the surface of steel castings
The sand sticking parts of the bolster and side frame are mainly concentrated near the inner sprue and the root
Bolster and side frame are important running parts on the bogie of rail freight car. They bear the gravity of
1.Sand sticking of cylinder block water jacket H003 cylinder block is an upgraded version of 52E cylinder block, in which
The liquid metal penetrates into the gap of molding sand, and after condensation, a layer of mechanical mixture of liquid
There is a layer of sand particles on the surface of castings that are difficult to remove, which is called
Features: the surface of the casting is bonded with a layer of molding material that is difficult to clean. There