Tensile fracture morphology of three grades of gray cast iron
The low magnification morphology of tensile fracture of three grades of gray cast iron is shown in Figure 1. It […]
The low magnification morphology of tensile fracture of three grades of gray cast iron is shown in Figure 1. It […]
Gray cast iron usually refers to the cast iron with gray section and the carbon mainly exists in the form
The tensile strength of ordinary HT250 at room temperature is slightly lower than the strength calibrated by its brand, which
Gray cast iron refers to the cast iron with flake graphite. The main components are iron, carbon, silicon, manganese, sulfur
The eutectic morphology of three grades of gray cast iron samples is shown in the figure. Eutectic clusters in gray
The matrix structure of three grades of gray cast iron samples is shown in the figure. It can be seen
The figure shows the graphite morphology and distribution of three grades of gray cast iron samples. It can be seen
The tension compression fatigue tests of three grades of gray cast iron are carried out on plg-100 high frequency fatigue
Gray cast iron characterized by flake graphite has certain strength, hardness, elastic modulus, shock absorption, wear resistance and thermal conductivity,
The low-frequency tension compression fatigue test of gray cast iron adopts MTS810 axial tension compression fatigue test machine. It uses
The tension compression fatigue test of gray cast iron mainly studies the effects of loading frequency and surface roughness on
Casting refers to pouring molten metal into the mold, cooling and forming to form a casting that meets the relevant
The test materials are three grades of gray cast iron, namely ordinary HT250, low alloy HT250 and HT300, in which
Because the brake drum works in the harsh environment with strong friction and complex alternation of cold and heat. Therefore,
Brake drum is an important component of automobile drum brake and one of the main security parts of automobile. It
Gray cast iron is an Fe-C-Si alloy containing graphite phase in pulse distribution. The annual output of castings in the
At present, with the development of marine engine to large-scale, the demand for large cylinder diameter, large tonnage and high-performance
(1) The graphite morphology of the three grades of gray cast iron samples is mainly type A, with a small
(1) The fatigue life curve of ordinary HT250 is shown in Figure 1. (2) The fatigue life curve of low
The gray cast iron cylinder body adopts the traditional horizontal pouring process, the sand core is dipped with coating respectively
The casting coating is composed of five basic components: refractory aggregate, carrier, binder, suspending agent and additives. With the development
The strength of gray cast iron is mainly determined by graphite shape, size, pearlite in matrix and ferrite proportion. With
The traditional method of high strength gray iron is to reduce the eutectic degree, to increase the austenite content and
The mass fraction of carbon in iron is higher than 2%, while that of silicon is between 1% and 3%.
In order to adjust the sand temperature, the air temperature must be considered. Although the curing reaction of resin sand
Furan resin can be divided into urea formaldehyde furan resin, phenol urea formaldehyde furan resin, formaldehyde sugar alcohol resin and
For the role of cold iron in the anti shrinkage process of castings, the sequential solidification theory and the equilibrium
In the past, riser design basically followed the principle of sequential solidification, which needs to meet the following three conditions:
The use of riser is one of the basic means to solve the shrinkage of casting. Although there are new
At present, there are many researches on the influence of metallurgical and molding factors on shrinkage cavity and porosity of