Microstructure and tensile properties of gray cast iron under low frequency thermal fatigue load
Gray cast iron is a common material for the production of ingot mold, chassis, sintering grate and industrial valves. Its […]
Gray cast iron is a common material for the production of ingot mold, chassis, sintering grate and industrial valves. Its […]
The samples of gray cast iron were treated by isothermal quenching and boronizing. The isothermal quenching process of gray cast
Aging treatment is used to eliminate the stress of castings, and the main factor affecting the stress elimination of castings
Heat treatment furnace is mainly divided into gas furnace, electric heating furnace and gas electric heating furnace. 1. Gas furnace
At present, the methods to eliminate stress in engineering include traditional natural aging, thermal aging and vibration aging. 1. Natural
The fatigue fracture process of metal mainly includes the process of fatigue crack nucleation and initiation, fatigue crack propagation and
1、 Metallographic observation Metallographic structure observation includes sampling, grinding, polishing, etching, cleaning, microscope observation and other steps. Metallographic specimen size
General materials contain some alloy compound phases. The existence of alloy compound phases enhances the matrix strength, hinders the crack
The fatigue performance of the material is affected by both the material itself and external factors. 90% of the fatigue
For cast iron, there will always be some unavoidable casting defects, such as shrinkage cavity and porosity. Casting defects have
Plg-100 high-frequency fatigue testing machine is used for high-frequency tension compression fatigue test of gray cast iron. The number of
The tensile strength of gray cast iron treated with 75 ferrosilicon inoculant is 6.5% lower than that of gray cast
The table shows the effects of the same alloying and different inoculants on the mechanical properties of gray cast iron.
The deformation of any material under external load will be affected by its own microstructure and properties and external environmental
Firstly, the fatigue crack nucleates at the stress concentration. Under the action of stress, the fatigue crack begins to expand.
The specific test process is as follows: 1.Use WAW-Y500 universal material testing machine to measure the tensile strength of the
For gray cast iron, its mechanical properties mainly depend on the matrix structure and flake graphite in it. The shape
The instantaneous fracture zone of fatigue crack is the area where the material is unstable and suddenly fractured. Due to
It is found that the fatigue properties of cast iron are not directly related to the conventional mechanical properties of
The fatigue crack growth region is the region of stable development after fatigue crack nucleation and initiation. Fatigue bands generally
As early as the 1940s, developed countries have studied the machinability of gray cast iron. Nowadays, the cutting performance of
The fatigue crack origin region is the region where the fatigue crack nucleates and initiates. The fatigue crack first nucleates
With the development of thin-walled engine block, the engine bears higher and higher pressure, which requires higher strength and fatigue
The machinability of gray cast iron is affected by different melting methods. From a large number of research and tests,
Gray cast iron has the characteristics of low cost, good casting performance and shock absorption, The key to the further
(1) Fatigue test of ordinary HT250 lifting Faraday compression The lifting diagram of tension compression fatigue limit of ordinary HT250
The tension compression fatigue fracture morphology of low alloy HT250 with different surface roughness is shown in the figure. Figure
In order to improve the properties of gray cast iron and deeply develop the application of gray cast iron, many
Results of tension compression fatigue test of low frequency gray cast iron Among the 8 samples of low-alloy HT250 low-frequency
Casting performance: it refers to some technological properties of whether the metal or alloy is suitable for casting, mainly including