Design and Optimization of Low Pressure Casting Process Parameters for Aluminium Alloy Battery End Plates
1. Introduction In recent years, with the rapid development of new energy vehicles, the demand for high-quality aluminium alloy battery […]
1. Introduction In recent years, with the rapid development of new energy vehicles, the demand for high-quality aluminium alloy battery […]
Abstract:This research focuses on the casting process of a double-suction impeller made from C95820 aluminum bronze, a material characterized by
This article focuses on the research of quantitative prediction of air entrainment defects in the casting filling process based on
Ductile cast iron, also known as nodular cast iron or spheroidal graphite iron, is a type of cast iron that
Gray cast iron is a fundamental material in many industrial applications due to its excellent mechanical properties, wear resistance, and
Abstract: Based on the practical courses for undergraduates, this paper explores product development through the integration of handmade clay (oil)
Abstract In order to comprehensively improve the motion and mechanical performance of the clamping unit in squeeze casting equipment, a
Spheroidal graphite iron (SG iron), also known as ductile iron, is renowned for its excellent mechanical properties, which make it
This article focuses on the analysis and improvement of nitrogen porosity defects in gray cast iron produced by iron –
Abstract: The structure of shell casting of a machine and the technical difficulties of investment casting were analyzed. The casting
Abstract This paper focuses on the optimization of the precision casting process for engine pre-combustion chamber inserts. Initially, the engine
Sand casting is time-tested manufacturing process used to produce a wide range of metal components. In recent years, significant innovations
This article focuses on the simulation of working stress and fatigue life of investment casting locomotive couplers. The coupler is
1. Introduction 3D printing, a recently emerged technology, has witnessed rapid development and expanding application ranges. The casting industry has a
Abstract: This article delves into the casting process of a steel casting for the exhaust end of an ultra-high pressure
Abstract: This comprehensive study delves into the formulation and role of various additives, including furan resin, curing agent, flame retardant,
Grey cast iron is a critical material in many industrial applications. However, its wear resistance can be a limiting factor
This article focuses on the analysis and improvement of nitrogen porosity defects in gray iron castings produced by the iron-mold
Abstract: This article delves into the casting process design for a large ductile iron bearing cover, addressing the common issues
Sand casting has been a cornerstone of metalworking for centuries, providing a versatile and cost-effective method for producing metal components.
This article focuses on the production process of large stainless steel volute castings. It details the product characteristics, mold design,
Abstract This paper primarily delves into the various defects encountered during the casting process of a gantry structure cylinder block
Abstract: This paper delves into the study of the investment casting process for K403 shell castings, which are crucial components
Sand casting is a versatile and widely used manufacturing process, but it comes with its own set of challenges. ZHY
This paper focuses on the die-casting process of the 9AT automotive transmission main housing. Through filling simulation, the influence of
Grey cast iron, known for its excellent machinability, vibration damping, and wear resistance, is widely used in various industries such
This article focuses on the casting process of the L21 front-end case. It analyzes the porosity problems encountered in production
Machinability refers to the ease with which a material can be cut, shaped, or finished using various machining processes. The
Abstract Sand casting is a widely used manufacturing process that involves pouring molten metal into a mold made from sand.
Al-Li alloys have attracted extensive attention in the aerospace and other fields due to their excellent properties such as high