Advantages of Dieless casting forming technology

1. Shorten the production cycle and improve the machining accuracy The mold less casting process adopts computer automatic processing, and the information processing process generally takes only a few hours. Compared with the traditional casting method, the mold less casting technology effectively shortens the production cycle of complex parts....

spacer

Principle and process of Dieless casting forming technology

1. Principle of Dieless casting forming technology Dieless casting is an advanced digital forming technology. Take the three-dimensional CAD model file of the casting as the carrier, use the created casting process database and casting simulation technology to optimize the model of the casting, complete the injection mold design...