Archives

Our Iron Foundry Manufacturing

Iron foundry manufacturing is very common in foundry industry manufacturing. We often see scenes like molten iron pouring. There is also sand mold we use for the iron foundry. There are many kinds of sand we can use in iron foundry process such as green sand, resin sand or...

spacer

Factors Influencing of Quality of Iron Foundry

Iron foundry usually made by using metal casting, due to the influence of various factors, there are holes, pinholes, slag, cracks and other defects. The quality of iron foundry mainly includes appearance quality, internal quality and service quality. First, appearance quality refers to the casting surface roughness, surface defect,...