Deformation analysis of compacted vermicular cast iron
The flatness of compacted vermicular cast iron platen surface is also very high. Therefore, the deformation of compacted vermicular cast
The flatness of compacted vermicular cast iron platen surface is also very high. Therefore, the deformation of compacted vermicular cast
Figure 1 shows the equivalent stress nephogram of vermicular cast iron pressure plate. It can be seen that the equivalent
The cloud diagram of solid phase distribution of vermicular cast iron is shown in Figure 1. From the solid phase
The pouring conditions of vermicular cast iron pressure plate are as follows: pouring temperature 1419 ℃, pouring speed 0.55m/s, pouring
In ProCAST, tetrahedral mesh model is commonly used for mesh generation. The quality of mesh usually affects the accuracy of
Vermicular cast iron automobile clutch pressure plate casting is a small casting, its overall structure is similar to a disc,
The steel castings produced by vertical casting scheme are shown in Fig. 1. The appearance quality of the castings is