Effect of normalizing temperature on mechanical properties of nodular cast iron samples
The tensile samples of room temperature nodular cast iron as cast and treated at different normalizing temperatures were tested at […]
The tensile samples of room temperature nodular cast iron as cast and treated at different normalizing temperatures were tested at […]
The figure shows the graphite morphology of cast iron alloy prepared with different addition amount of spheroidizing agent. Among them,
The figure shows the matrix structure of as cast ductile iron. It can be seen from figure a that the
Taking nodular cast iron as the research object, the influence of mechanical vibration on the microstructure and properties of nodular
For the liquid metal casting process, the interval between pouring of two metals is very critical: the interval is too
The vibration solidification equipment used in the vibration lost foam casting is a two-way electromagnetic vibration table with the model
Experimental raw materials mainly include metal raw materials, non-metal raw materials and modeling materials. Metallic materials mainly include cast pig
Qi Jiyu found that the material, derusting method, thickness and metal liquid temperature of the diaphragm may affect the bonding
When high chromium cast iron is as cast, eutectic carbide (M7C3) with broken network distribution exists in its microstructure. The
At present, the following methods are usually used to solve the problems of coarse structure and low mechanical properties in
Due to the different actual conditions of the solution condensation process, the carbide morphology, size and quantity of high chromium
The microstructure was observed by optical microscope (OM), the microstructure was observed by scanning electron microscope (SEM), the carbide type
1.M7C3 eutectic carbide: when the CR / C ratio is greater than 3.5, high hardness eutectic carbide (Fe, Cr) 7C3
In 1965, China began to research and apply the lost foam casting technology, which is one of the countries that
The wear caused by the severe friction of the brake drum in the braking process and the fatigue cracking caused
The high chromium cast iron carbon steel bimetallic casting lining plate was installed in the wet ball mill, and the
There are many tests for statistical distribution, such as KS test, chi square test, etc. from the perspective of graphics,
1.Soil abrasive particles and medium The aggravation of wear at each wear part of tractor track shoe is closely related
As we all know, cast iron alloy is a multi-element alloy composed of iron, carbon and silicon. When the carbon
As shown in Figure 1, the left mold cavity is filled with high chromium cast iron liquid first, then flows
The composite thickness range of high chromium cast iron and carbon steel is shown in the figure below: According to
The intermediate diaphragm / horizontal vertical pouring refers to that the mold is molded at the horizontal position, the cavity
Using the vertical pouring process, it is necessary to insert an intermediate diaphragm at the junction of the two metals.
Lost foam casting technology, also known as full mold casting, is a casting method in which the foam pattern with
Fig. is a picture of the effect of modification on the microstructure of as cast high chromium cast iron: Fig.
The creep effect of rare earth was found in the process of treating nodular cast iron with rare earth, but
When high chromium cast iron is as cast, its matrix structure is austenite. The austenitic structure has good plastic toughness,
The research work mainly serves the ZHY casting technical transformation project and takes meeting the process production requirements as the
The theoretical basis of casting process CAD system design is the process design method used in the actual production of
The typical solidification structure of hypoeutectic high chromium cast iron is primary austenite and reticular eutectic carbide (M23C6 or M3C