Trial production of alloy casting in rapid investment casting
The diffuser shell adopts high strength ceramic shell process, which is composed of surface layer, transition layer and back layer. […]
The diffuser shell adopts high strength ceramic shell process, which is composed of surface layer, transition layer and back layer. […]
SLS rapid investment casting generally needs three steps: SLS prototype firing, wax impregnation post-treatment and investment casting. Because there is
Through the analysis of the research status at home and abroad, combined with the existing experimental research, and finally according
ProCAST simulation software was used to simulate the gating system, and the temperature field changes and casting defects during filling
In the process of rapid investment casting, due to the different rapid prototyping process, the corresponding casting process scheme is
UG software is used to save the designed initial gating system file in x-t format and import it into the
SLS sintering process and material types have a great influence on the sintering results. Most scholars study the influence of
Mainly through the trial production of rapid investment casting process, including: gating system design; casting simulation pretreatment settings; numerical simulation
1.Technical requirements For the technical requirements of metallographic structure, most customers’ products are basically consistent with those recommended in technical
With the continuous rise and popularization of 3D technology, China’s manufacturing industry has gradually achieved upgrading, especially in the mold
The size correction of the typical complex diffuser was completed by using magic software. Through the analysis of the size
Rapid casting (QC) is a new technology formed by combining SLS, SLA, FDM and traditional casting technology. The application object
Select a mine φ 12.2 m × The middle ring liner of 11.0 m autogenous mill is taken as the
Combined with the rule of dimension error transfer from CAD model to one-time wax impregnation, the dimension shrinkage in X
Traditional investment casting is also known as “wax loss casting”. Because of the high dimensional accuracy and surface quality of
Based on the rule of dimensional error transfer and reverse engineering, the 3D digital scanning of complex parts after one
Composition analysis of high chromium cast iron At present, the research of high chromium cast iron focuses on hypoeutectic or
Due to the complexity of squeeze casting process, it is very difficult to measure the internal pressure of squeeze casting
In view of the influence of different post-treatment on the surface quality of the specimen, considering the low surface strength
Analysis of casting structure and casting process The main body of the lower half casting of the rear cylinder is
For the interface heat transfer with pressure, there is a definite relationship between the interface heat transfer coefficient and the
In the experiment, the dimension deviation is used as the measurement index of the dimension accuracy of the specimen. The
For the SLS fired specimens, the specific dimensions are shown in Figure 1. The size of the sample for selective
The main parameters involved in squeeze casting process include: applied pressure, pouring temperature, initial mold temperature and coating thickness. These
The experimental measurement of interface pressure and internal temperature of squeeze casting and the calculation of interface heat transfer coefficient
The process parameters of SLS were predicted as follows: temperature 95 ℃, laser power 30W, powder layer thickness 0.14mm, scanning
A 1000KN hydraulic press was used to apply the external pressure of squeeze casting, and a medium frequency induction aluminum
As for specimen selection, Wang Danni of Wuhan University of science and technology used finite element analysis and BP neural
The core idea of the optimization method is that the solution of the heat transfer coefficient of the casting die
The transformation of alloy from liquid to solid is called solidification, during which casting defects are concentrated. In the process