How to deal with the insufficient strength of casting coating
The strength of casting coating can not be divided into two situations: one is the normal drying strength, the other […]
The strength of casting coating can not be divided into two situations: one is the normal drying strength, the other […]
The anode steel claw for electrolytic aluminum is also called electrolytic claw. There are parallel three claws, four claws, three-dimensional
Modern engines have very strict requirements on cleanliness. For cylinder block (cylinder head) castings, only a few grams (g) of
Calculation of resistance cross section The total sectional area a can be calculated according to the following formula =Q/KTL in
Defect characteristics and detection methods It is often found after sand cleaning or sand blasting of castings that the layered
The pouring system is a channel to guide liquid metal into the mold cavity, which is composed of sprue cup,
Features: The appearance of the casting is incomplete, with a crack like gap or broken flow, and the metal edge
The function of sand core is to form the inner cavity, hole of casting and the part that can’t produce
Sand inclusion refers to that there is a layer of metal lump or sheet on the surface of the casting,
7 Discoloration and spots (1) characteristics: There are different colors and spots on the casting surface. (2) Causes: ① Improper
Dimensional tolerance of castings refers to the difference between two allowable limit dimensions of nominal dimensions of castings. Within two
Features: small holes filled with mold (core) sand inside or on the surface of defects are called sand holes. If
Production conditions, structure and technical requirements of fixture Product production nature – mass production Part material – 35Cr The part
Green sand is composed of original sand, clay, additives and water in a certain proportion. The commonly used feeding sequence
Lost wax casting is now called investment casting. It is a kind of casting technology with little or no cutting.
Casting can also be divided into gravity casting and pressure casting according to the pouring process of liquid metal. Gravity
Usually in the inner surface or hot spot of the casting, such as the water jacket cavity of the cylinder
4.Casting deformation (1) characteristics: ① Overall deformation or local deformation; ② the geometric drawing of the die casting is inconsistent.
Clay sand mold can be divided into wet mold, dry mold and surface drying mold. The main differences among the
In casting production, mold is very important. All kinds of process knowledge we talked about before should be included in
The material used to make sand mold is called molding material, the material used to make sand mold is called
Using riser, chill and cast steel bar to obtain high quality castings is a common technological measure in foundry production.
Sand hole is also a common defect of cylinder block (cylinder head) casting, which is often found on the upper
For the same alloy, whether the hub cracks or not often depends on the hub structure, process parameters and mold
1 casting strain (1) characteristics: ① Along the opening direction, the surface of the casting shows a line like scratch
Machine modeling — the molding machine completes the main actions of sand filling, compaction and touching during the molding process.
(1) According to the position of the choke section A closed gating system The closed gating system refers to the
Features: the fracture surface of the casting is gray black, and the mechanical properties are obviously low. Through metallographic examination,
Casting is the process of melting metal into a liquid that meets certain requirements and pouring it into the mold.
Gating system design: 1.Design of sprue cup (1) Sprue cup shape The shape of sprue cup can be divided into