Microstructure analysis of graphite morphology and distribution in nodular cast iron
Fig. 1 shows the microstructure SEM of three groups of ductile iron samples. It can be seen from the figure […]
Fig. 1 shows the microstructure SEM of three groups of ductile iron samples. It can be seen from the figure […]
General materials contain some alloy compound phases. The existence of alloy compound phases enhances the matrix strength, hinders the crack
For cast iron, there will always be some unavoidable casting defects, such as shrinkage cavity and porosity. Casting defects have
The table shows the effects of the same alloying and different inoculants on the mechanical properties of gray cast iron.
The deformation of any material under external load will be affected by its own microstructure and properties and external environmental
For gray cast iron, its mechanical properties mainly depend on the matrix structure and flake graphite in it. The shape
The instantaneous fracture zone of fatigue crack is the area where the material is unstable and suddenly fractured. Due to
The fatigue crack growth region is the region of stable development after fatigue crack nucleation and initiation. Fatigue bands generally
The fatigue crack origin region is the region where the fatigue crack nucleates and initiates. The fatigue crack first nucleates
(1) Fatigue test of ordinary HT250 lifting Faraday compression The lifting diagram of tension compression fatigue limit of ordinary HT250
The tension compression fatigue fracture morphology of low alloy HT250 with different surface roughness is shown in the figure. Figure
Results of tension compression fatigue test of low frequency gray cast iron Among the 8 samples of low-alloy HT250 low-frequency
The low magnification morphology of tensile fracture of three grades of gray cast iron is shown in Figure 1. It
The tensile strength of ordinary HT250 at room temperature is slightly lower than the strength calibrated by its brand, which
The eutectic morphology of three grades of gray cast iron samples is shown in the figure. Eutectic clusters in gray
The figure shows the graphite morphology and distribution of three grades of gray cast iron samples. It can be seen
The tension compression fatigue tests of three grades of gray cast iron are carried out on plg-100 high frequency fatigue
After the above WPS preparation, WPQR welding procedure qualification test shall be carried out to determine the WPS process reliability.
The low-frequency tension compression fatigue test of gray cast iron adopts MTS810 axial tension compression fatigue test machine. It uses
Generally, the hardness of cylinder liner in the qualified layer is hb225 ~ HB240, and the overall hardness difference of
The tension compression fatigue test of gray cast iron mainly studies the effects of loading frequency and surface roughness on
As shown in Figure 1, cut the metallographic sample close to the crack source, and then conduct rough grinding, fine
The test materials are three grades of gray cast iron, namely ordinary HT250, low alloy HT250 and HT300, in which
1. Improvement of gating system 1.1 The intermediate injection water inlet is improved to the top injection water inlet At
Single point fatigue test is applicable to the service of metal components under rotating bending load at room temperature, high
A large number of experimental studies have proved that in general, the higher the purity of metal, the better its
The valve body of seawater butterfly valve with nominal size of DN1200 is made of 00Cr25Ni7Mo4N, with a gross weight
(1) Cause analysis of formation of porosity in invasive casting. The total amount and rate of gas produced by molding
In fact, the fatigue failure of materials is mainly due to the irreversible change of the material structure. When the
The flywheel housing is placed vertically in the lost foam casting sand box (as shown in Fig. 1), and there