(1) According to the position of the choke section A closed gating system The closed gating system refers to the
(1) According to the position of the choke section A closed gating system The closed gating system refers to the
Gating system design: 1.Design of sprue cup (1) Sprue cup shape The shape of sprue cup can be divided into
1.Casting shrinkage There are many factors that affect the casting shrinkage, such as the type and composition of the alloy,
Casting features: 1.Casting has a wide range of adaptability, great flexibility, product requirements and various working conditions. It can manufacture
1.Improve the structure of boss, flange and rib plate that hinder the lifting The boss (LAP), flange, rib plate, etc.
There are many advantages as a result of the technology Foam Lost, not to mention just a few: – Energy
In this technology, is a stock made from foamed polystyrene (EPS). Foaming of the polystyrene out not only to patrons
In the past years, the Lost Foam process is widely used worldwide. According to the data published by Vulcan, in
During sand mold casting, in order to be used repeatedly sand casting pattern are made of relatively tough materials. There are many