Study on sand casting technology of automobile engine parts
Three kinds of Dieless manufacturing processes, including laser selective sintering of coated sand, laser selective sintering of PS powder and […]
Three kinds of Dieless manufacturing processes, including laser selective sintering of coated sand, laser selective sintering of PS powder and […]
(1) The minimum sectional area of gating system shall be determined. The minimum area of gating system is generally calculated
At present, sand castings inside passenger car engines mainly include cylinder block, cylinder head, bearing cover, exhaust pipe, valve cover,
(1) Determine the position of the pattern in the casting sand mold Select a flat bottom plate and a sand
As the water glass sand mold core is impacted and surrounded by high-temperature liquid metal, and the working conditions are
According to empirical parameters, when the wall thickness of impeller investment casting sand casting is > 40 mm, the minimum
Figure 1 and Figure 2 show the graphite structure of HT250 and HT200 gray cast iron under the conditions of
According to the three carbon source calculation models based on three types of sand casting process parameters, the total carbon
The carbon emission of sand casting parts is determined by its casting process. The typical sand casting production process goes
Combined with the research status of relevant fields, sand casting process has a significant impact on the sustainable development of
As people pay more and more attention to industrial pollution, environmental laws and regulations in many countries are becoming more
The solidification process of sand castings is directly related to the shrinkage cavity, porosity and stress concentration of sand castings.
1. Sand core design of sand mold casting The core is made of furan resin self hardening sand. Because the
The spiral case is made of QT500-7, and its chemical composition is shown in the table. The production nature of
After the simulation calculation is completed, enter the visual viewer post-processing interface, observe the dynamic change of liquid metal temperature
Compared with other metal castings, sand casting has the advantages of low cost, simple production process and short production cycle.
1. Simulation analysis of liquid metal filling process The filling state and temperature distribution at different stages of liquid metal
The process of rapid sand casting technology to realize the rapid manufacturing of parts is as follows: establish the three-dimensional
According to the above anti gravity test results, the differential pressure sand casting process was selected to pour the actual
The wall thickness of the hatch sand casting is 2 mm, and the dimensional accuracy requirements are high. It is
The hatch sand castings are sand castings with overall wall thickness of 2 mm. There is no report on the
The hatch sand casting is a key structural member of aluminum alloy for aircraft. The outline dimension of fad hatch
1. Sand mold casting process scheme of nodular cast iron Nodular cast iron sand castings are produced in single piece
The gross weight of the frame used in the simulation is 60t, the weight of the pouring riser is 30t,
The figure shows the results of shrinkage porosity after solidification of sand casting frame, and the criterion of casting shrinkage
In the numerical simulation of solidification process of sand castings, the thermophysical parameters of the mold are one of the
The figure shows the solidification fraction of the sand casting frame at different times. It can be seen that the
During the solidification and cooling process of sand castings, the shrinkage capacity of each part is different due to the
Numerical algorithm is the mathematical basis of numerical simulation of sand casting process. There are three common numerical calculation methods:
1. Production of heat subsidy for sand casting Mix the powdered heating material and binder evenly according to the required