Liquid segregation of 7075 alloy in rheo squeeze casting
By analyzing the metallographic structure of the parts successfully manufactured by rheo squeeze casting, it is found that liquid phase […]
By analyzing the metallographic structure of the parts successfully manufactured by rheo squeeze casting, it is found that liquid phase […]
Injection system is one of the key subsystems of squeeze casting equipment. In the production process of squeeze casting, the
In recent years, with the promotion of energy saving and emission reduction, light weight and environmental protection in China, more
Figure 1 shows the metallographic structure of different parts of 7075 alloy wheel extrusion casting. It can be seen from
Cast iron is melted in the atmosphere, and a variety of oxides will be brought into various charges. However, the
The clamping and locking mechanism is mainly used to install the squeeze casting mold for clamping, opening and ejection. The
1. Strength analysis The comparison between the strain caused by temperature (including preload and gravity) and that under all loads
As shown in the figure, the die structure of squeeze casting includes upper and lower die, die base, die core,
(1) Pouring of semi-solid alloy melt: the semi-solid slurry prepared by lspsf process is poured into the barrel of semi-solid
The quality of wheel shaped rheo squeeze casting parts is closely related to the extrusion filling speed, pouring temperature, mold
360° The whole cylinder is used for the analysis of the low pressure inner casing with volute inlet steam, and
The key of semi-solid processing technology is to form fine semi-solid spherulites with high degree of equiaxed spherulites by certain
In order to improve the quality of wheel shaped squeeze casting parts, the process parameters of different extrusion filling speeds
High strength ductile iron is an important engineering structural material. Although it came out late, it has good machinability and
(1) Reduce the level of non-metallic inclusions in castings. The main purpose is to improve the purity of liquid steel.
Under the condition that the pouring temperature is 630 ℃ and the extrusion filling speed is 0.4m/s, the mold temperature
Since the thixotropic properties of semi-solid metals were discovered by American scholars in the 1970s, semi-solid processing technology has been
Under the condition of keeping the die temperature at 160 ℃ and high extrusion speed of 0.4m/s, the pouring temperature
Squash casting is one of the typical casting processes which can eliminate the porosity defects, and a new material processing
According to the specific parameters of semi-solid vertical squeeze casting machine, combined with the laboratory test data, the process parameters
With the increasingly fierce market competition, the quality requirements of engine products are higher and higher, especially the requirements of
The preparation of metal semi-solid slurry is the key link of its processing technology, which is directly related to the
The residual stress of cylinder head castings has always been an important problem in cylinder head casting. After casting, due
The process of numerical simulation of AnyCasting software includes: firstly, the pre-processing is carried out by any pre, including the
With the rapid development of computer technology, solidification simulation technology is also developing very rapidly. The solidification simulation CAE and
Based on the theory of numerical simulation and fluid mechanics, the equations of solidification heat transfer are established Momentum conservation
1. Casting process design According to the structure of the casting, the three box molding process is adopted, as shown
According to the different materials, shapes and sizes of the parts, a variety of different squeeze casting forming processes are
The semi-solid 7075 alloy melt is different from the traditional liquid alloy ① Semi solid alloy melt has good fluidity,
The structure of the water-cooled steel brick casting is complex (see Figure), and the water pressure test of 0.5MPa is