Selection of riser size and location for large gray iron castings
The use of riser is one of the basic means to solve the shrinkage of casting. Although there are new
The use of riser is one of the basic means to solve the shrinkage of casting. Although there are new
1) The reasonable design of the riser, the heat preservation sleeve and the casting pouring system constitute the riser system,
In the casting of automobile parts, the wheel casting is a little different. Because it needs to meet a series
For the convenience of research, the pouring system is classified into top pouring, bottom pouring and step pouring according to
At present, there are many researches on the influence of metallurgical and molding factors on shrinkage cavity and porosity of
Due to the use of lightweight aluminum alloy materials, compared with the steel and cast iron used before, automatic production
Because the equipment is the core platform for the implementation of the technology, and the composite squeeze casting method is
1. Definition of composite squeeze casting Direct squeeze casting technology pressure directly acts on the surface of liquid metal, the
The process of loading metal raw materials with mold and other equipment to produce plastic flow to produce products that
The main function of the squeeze casting die in the forming process is to complete the liquid metal forming, to
Hot spots 1: reduce or eliminate the casting defects of lead alloy in EPC The biggest problem of making lead
In the early application of squeeze casting technology, the transportation of molten metal is basically manual transportation and mold filling.
A large number of researches and applications have been carried out on the squeeze casting forming technology in foreign countries.
1) Prediction of shrinkage porosity and porosity Shrinkage cavity and shrinkage porosity are the holes that appear when the temperature
1. Application case carbon emission estimation The material of a casting is HT150, which is produced in batches. As shown
With the rapid development of economy, the domestic demand for large and complex parts is increasing in the fields of
1. Energy consumption of sand casting production system The carbon emission of sand casting production system is related to energy
Numerical simulation of casting filling is to analyze the heat transfer phenomenon and forming ability of high temperature liquid metal
China’s automobile industry is booming and has become the pillar industry of national economic development. However, China’s automobile industry still
1. Carbon emission source of sand casting production system A large amount of waste gas produced by sand casting production
Rapid Prototyping technology relies on the point by point accumulation forming of materials, which is not restricted by the manufacturability
The casting process of part structure usually refers to that the structure of the part itself should meet the requirements
Features: Coarse graphite: the size of graphite in the metallographic structure is very large, or there is massive graphite, and
Features: Poor lower core (core deviation, core dropping, sand squeezing and core breaking) Causes: A. Mask is not adjusted well,
When the wall thickness of high-temperature alloy castings such as adjusting piece and sealing piece is changed from 1.1mm to
Features: The white cast is hard and brittle, and it is difficult to break and turn white Causes: A. Casting
1, Characteristics There are defects in some parts of the casting, which often appear in the thin-walled part, the farthest
Fast graphite fragmentation The broken fast graphite is a kind of deformed graphite which often appears in the large end