Application case of 3D printing technology in sand casting
The components of an automobile steering gear are shown in Figure 1. The sand casting has complex structure, many processing […]
The components of an automobile steering gear are shown in Figure 1. The sand casting has complex structure, many processing […]
The emergence of 3D printing technology has certain advantages in additive manufacturing. At present, 3D printing technology has a very
1. Self development Sand casting is the basic industry of industry and has an irreplaceable position. From high-end industrial machinery
The traditional sand mold casting mode is to use mold modeling and sand mold combined pouring to form sand mold
At the same time, the teaching content of spiral casting is optimized by consulting the teaching materials in the early
Casting is an important teaching module of metalworking practice course. Its teaching content is composed of sand casting, lost foam
The variation law of interfacial heat transfer coefficient of typical ZL101 Aluminum alloy ring sand castings with height of 150
Based on the temperature field data measured by pouring experiment and the established matlab inverse calculation program, the interface heat
Industrial rotary kilns are widely used in cement, metallurgical pellets, active lime, chemical and other industries. The supporting roller is
1.Optimize the sprue The vertical sprue is changed to a “2” shape sprue, that is, a bend is set on
According to the structural characteristics of the product and referring to the results of similar products after production, two process
The steam turbine end cover is used to seal the steam in the condensate. It has high requirements on the
The setting of simulation pretreatment mainly includes the selection of simulation items, material selection rules, heat exchange conditions, pouring conditions
In order to make the simulation results compare with the measured temperature curve, the established geometric model should be the
Combined with the actual solidification process of sand castings, the three-dimensional model is established through UG, and ProCAST is used
According to the macroscopic definition formula of interface heat transfer coefficient, it is necessary to know the temperature T1 of
The temperature data at the thermocouple measured in the experiment are sorted into the data form required by the inverse
The three groups of pouring test temperature data of ring sand casting during solidification are as follows: Figure 1, figure
This link should focus on the inspection of personnel skills and experience. The operator’s work certificate can be checked. At
The temperature data measured in the solidification process experiment is the basis for solving the interface back calculation. Therefore, it
These two processes are basically similar, which are the basis of the whole casting process and directly affect the box
1. The traditional sand casting method has low precision and cannot meet the production of complex parts such as turbine
The links are mainly from the molding, core making, box matching, pouring, cleaning and heat treatment processes. Firstly, the heat
18PA6B sand mold casting crankcase is made of nodular cast iron, with a gross weight of about 13T. Resin sand
Because sand casting is a special process, with many hidden links and collective operation mode, some processes cannot be directly
For each sand casting process scheme, sufficient experimental preparations need to be carried out before the temperature measurement experiment, which
18PA6B sand casting diesel generator sets are widely used in domestic nuclear power plants, such as CNNC Jiangsu Tianwan nuclear
In order to solve the interface heat transfer coefficient between sand casting and mold / core through numerical back calculation,
In the process of metal solidification during sand casting, the solidification volume contraction of metal and the thermal expansion of
According to the actual production situation of sand casting, on the basis of summarizing and analyzing the theory of sand