Analysis of the original solidification process of steel castings
Figure 1 shows the temperature distribution results of the hook body 5 s after it starts to solidify. The solidification […]
Figure 1 shows the temperature distribution results of the hook body 5 s after it starts to solidify. The solidification […]
Figures 1 to 4 show the simulation analysis results of the mold filling process of hook steel castings. Figure 1
The coupler body and casting process are modeled by proe and exported by Parasolid interface file format XT mesh file,
The total number of cracks in the motor shell produced by furan resin sand casting process is about 70, while
The machinability of materials refers to the difficulty of cutting the excess part of materials to obtain qualified parts. Therefore,
According to the previous casting simulation results, it is found that the process riser of the steel casting plant is
The sand inclusion casting defects of steel castings are relatively serious, because the proportion of product scrapping caused by sand
The coupler body of type 17 coupler is a complex medium and small steel casting with the overall size of
It mainly simulates and optimizes the process of two parts: 17 coupler body and 16 coupler tongue, which are important
In view of the problems and deficiencies existing in the existing furan resin sand process, motor shell sand mold casting
The mechanical properties and machinability of gray cast iron samples for engine cylinder block were tested, and the microstructure of
① Analysis on the original pouring system of motor shell See Fig. 1 for the original pouring system of motor
There are relatively few enterprises and scientific research institutions engaged in the production and research of wet clay sand railway
Sand casting process simulation technology introduction in the process of national economic development, sand casting industry, as an important part
Before the proportion of molding sand is proposed, the basic range of molding sand properties should be determined according to
The green molding clay sand used in railway steel castings is mainly made of raw sand, bentonite, starch additives and
Cast iron is the most widely used basic material in metal materials and plays an important role in casting alloys.
The orthogonal experiment will be designed, the riser height is set as the independent variable, and other process parameters remain
(1) Ultrasonic flaw detection of cast steel joints can not cover all flaw detection areas, nor can it completely and
“Energy conservation” and “environmental protection” are important issues facing China in development, and realizing sustainable development is our basic national
Railway development is closely related to people’s life and national development. With the sixth speed increase of railway, railway freight
Casting sand inclusion defects are directly related to production process, mold, sand mixing, molding, core making, lower core box, pouring
Taking the sand mold casting of the mud pump body as the research object, firstly, the gating system, feeding system
Figure 1 shows the simulation results of temperature field at each time during solidification of mud pump body in sand
Traditional nondestructive testing methods include ultrasonic testing, acoustic emission testing, magnetic particle testing and radiographic testing. Magnetic particle flaw detection
Discussion on quality evaluation standard of cast steel joints: (1) For the flaw detection of castings, special attention can be
The defect distribution of sand castings after processing is shown in Figure 1, figure 2 and figure 3. The sand
Aiming at the problems of coarse structure and low mechanical properties of cast iron alloy lost foam casting, vibration lost
(1) Through the non-destructive testing of 24 cast steel joints, it is found that the distribution of casting defects seems
According to the flaw detection results, there are many casting defects in the cast steel joints, and many casting defects