Numerical simulation of solidification process of track shoes in Lost Foam Casting Process Based on ProCAST
Crawler shoe is the key component of roadheader walking mechanism, which is connected by pin to form crawler shoe chain.
Crawler shoe is the key component of roadheader walking mechanism, which is connected by pin to form crawler shoe chain.
The segregation behavior of impurity elements needs to be analyzed from the aspects of solidification thermodynamics and kinetics. From the
According to the data in Table 1, the segregation position of each element along the longitudinal direction can be further
The contents of impurity elements at different positions in A356 aluminum alloy wheel hub by reverse squeeze casting are shown
The test material is A356 aluminum alloy, and its chemical composition is controlled according to American Standard b108-03a. A heavy
The top plate casting is an important part of the supporting transportation equipment for metallurgical vehicles. Its structure is shown
1 Mold Design According to the overall dimension of the product, the size of sand box is 550 mm ×
1 Production Process The production process is shown in Fig. 1 ~ 5, including coating spraying, coating drying, core setting,
The casting process of crusher frame products is relatively mature, and the process design ideas are generally similar, and the
The cutterhead body produced by the company is made of ZL104 material. The cutterhead body is used to install the
As for the development of vermicular graphite cast iron technology, in 1948, the Americans applied it. However, due to the
In the process of solid solution, the alloy elements are dissolved into the base metal, the hardness and strength of
According to the above research and analysis, it is concluded that the best T6 heat treatment process for rheo SQUEEZE
A number of heat-treated samples with the size of 15 × 15 × 15mm were selected from the successful parts.
The results show that the strength of 7075 rheo squeeze casting parts can be greatly increased by aging treatment. The
The Brinell hardness values of 7075 rheo squeeze casting samples after solution treatment at different time were counted in the
After determining 475 ℃ as the best solution temperature, four 15 × 15 × 15mm heat-treated samples were taken from
It can be seen from the metallographic structure figure 1 after solution treatment at different temperatures for 2 h that
Hardness test is the most simple and easy method in mechanical property test. In order to replace some mechanical property
The DSC thermal analysis curve of 7075 aluminum alloy was tested in the experiment. According to the thermal analysis curve,
(1) The experimental scheme and process. The slurry was prepared by lspsf semi-solid pulping process, and the 7075 aluminum alloy
The effect of injection specific pressure on the mechanical properties of 7075 alloy by rheo squeeze casting is shown in
The volume of 7075 aluminum alloy shrinks when it crystallizes. For squeeze casting, solidification under pressure will increase the undercooling
Through lspsf process, connecting with the special semi-solid vertical squeeze casting equipment developed by the laboratory, and adopting reasonable process
In the middle part of the workpiece, take a test bar with a diameter of 6 mm according to the
1. Defect analysis (1) The rib plate of the cylinder body forms a grid shaped geometric hot spot with the
By analyzing the metallographic structure of the parts successfully manufactured by rheo squeeze casting, it is found that liquid phase
Figure 1 shows the metallographic structure of different parts of 7075 alloy wheel extrusion casting. It can be seen from
As shown in the figure, the die structure of squeeze casting includes upper and lower die, die base, die core,
The quality of wheel shaped rheo squeeze casting parts is closely related to the extrusion filling speed, pouring temperature, mold