Gray cast iron is a common raw material of cast iron
Cast iron is the most widely used casting metal material in modern industry. The applications of cast iron in various […]
Cast iron is the most widely used casting metal material in modern industry. The applications of cast iron in various […]
As the most important output component of the shearer gear transmission system, the planet carrier has a complex structure and
①When using polystyrene foam in white mold manufacture, its density is very small, and the labor intensity of the operators
In view of the casting defects of the compressor diaphragm in the casting process, the mechanical properties of the casting
The fire-resistant coating for lost foam casting includes refractory aggregate, carrier (solvent), suspending agent, binder and other additives. ① Refractory
One layer of refractory coating hung on the outer surface of the foam plastic model is one of the three
Cast diaphragms are the main stator components in centrifugal compressors. According to the different arrangement positions and functions of cast
The process flow of lost foam casting is divided into two parts: white area and black area. (1) the process
lost foam casting process technology, usually referred to as EPC in English, is also known as gasification mold casting or
1. Impact performance After the impact test is completed, the impact absorption rate of bearing pedestal will change with the
1. Test materials and casting process parameters Combined with the scientific casting process and methods, the properties of casting samples
As we all know, bearing pedestal is an important part of modern machinery and plays an important role in the
The bearing pedestal can fix the bearing, support the operation of the bearing, and bear the pressure brought by the
At present, the coupler knuckle used in the couplers of China’s railway freight cars is cast coupler knuckle. The cast
The process selection of rare earth inoculating gray cast iron depends on the adding method of inoculant, mainly including flat
According to the principle of conventional parting surface selection: the parting surface shall be as simple as possible, and the
Forged coupler knuckle is an important part of the coupler and draft gear of freight cars. Forged coupler knuckle is
1.Charge The quality of furnace charge mainly depends on the content of trace elements in raw materials. The trace elements
Oxygen mainly exists in the form of oxidation inclusions in gray cast iron. Gray cast iron samples with different oxidation
Sulfur can cause “hot brittleness” of cast iron during smelting of gray cast iron and reduce the corrosion resistance, welding
As a high-efficiency inoculant, rare earth has always occupied an important position in the application of inoculant, mainly because it
With the development of industrialization in China, ductile iron has become the main metal material in industrial production due to
Spheroidized elements usually have the following common properties: (1) In gray cast iron, the solubility of elements in molten iron
The creep effect of rare earth was found in the process of treating nodular cast iron with rare earth, but
Adding rare earth elements into gray cast iron can significantly improve the mechanical properties of gray cast iron, such as
The molten steel of steel castings has high melting point, poor fluidity, large shrinkage and easy oxidation. Therefore, the gating
The strength of gray cast iron mainly depends on graphite and matrix structure. With the increase of carbon equivalent, the
In the past, similar steel castings used the core assembly molding, and the size of the sand core is relatively
The steel casting of splay saddle saddle head is the first suspension bridge for both highway and railway in China,
Since the 1980s, the rare earth industry has developed rapidly. Whether abroad or at home, the application technology of rare