Milling degree of flat Graphite cast Iron with PCBN Cutter
PCBN cutters can be used for rough machining to improve machining efficiency, or finish machining to improve surface quality. This […]
PCBN cutters can be used for rough machining to improve machining efficiency, or finish machining to improve surface quality. This […]
The source of cutting force is the resistance of the tool to overcome elastic deformation, plastic deformation and friction. The
The experiment was carried out in the DAEWOOACE-V500 vertical machining center. The schematic diagram of orthogonal milling is shown in
In orthogonal turning, only one straight cutting edge is involved in the cutting, and the cutting edge is perpendicular to
There are many commonly used constitutive equations of metallic materials, including Power-Law model, Zerilli-Arstrong model, Johnson-Cook model and so on.
1. Data processing of tensile experiment. Figure 1 shows the stress-strain curve of static tensile test. As can be seen
Figure 1 shows the small Hopkinson pressure bar equipment used in this experiment. Figure 2 is a schematic diagram of
Because the chromium white cast iron used in the experiment is brittle material and has not been heat treated, the
Impact toughness is an important index of large wear-resistant plate. It refers to the ability of material to absorb plastic
It can be seen from Figure 1 that compared with the normal pressure, the hardness of the alloy can be
Different from equilibrium solidification, the solidification process of alloy melt under pressure is controlled by nucleation and subsequent crystal growth.
It has been proved that different types of carbides have different hardness. The purpose of different casting processes is to
Besides discussing the interface structure, which is the mechanism of atom stacking and crystal morphology, we also need to discuss
Crystal growth is a process in which the atoms in the liquid phase migrate and stack to the surface of
From the point of view of thermodynamics, primary carbides should only exist in hypereutectic alloy. But in fact, it can
Because the composition of low chromium white cast iron alloy 1 is far away from eutectic point, the carbides are
In the solidification process of Hypoeutectic chromium white cast iron, the primary phase is austenite, the carbides in the solidification
The total amount of carbides, eutectic carbides and primary carbides in alloy 2 are shown in the figure. The content
In order to better compare the solidification structures of different sampling positions under different pressures, the solidification structures of top,
(1) Solidification structure of specimens at different positions under atmospheric pressure The solidification structure of alloy 2 under normal pressure
The results show that the pressure, fluidity and cooling rate of liquid metal at different positions are different during solidification.
The stability of solid-liquid interface affects the morphology of microstructure and determines the final properties of materials. The expression of
The relationship between pressure and solute diffusion coefficient can be described as follows Where: DP — solute diffusion coefficient under
Through the characterization and analysis of the morphology of the above hypoeutectic alloy 1 # eutectic structure, the eutectic morphology
Because the primary phase in the solidification structure of alloy 1 is austenite, the eutectic austenite in the divorced eutectic
Through the quantitative characterization of eutectic structure under different pressures, it can be seen that the morphology of each phase
The metallographic structure shown in the figure is the metallographic structure photo of near eutectic alloy 2. It can be
1. Hardness test (1) Macrohardness Thbrv-187.5 electric broville hardness tester is mainly used for macro hardness analysis of samples. As
1. Sample preparation (1) Sample grinding and polishing Use pg-2da metallographic sample polishing machine to pre grind the sample with
1. Alloy melting The alloy was melted in 500 kg medium frequency induction furnace in air atmosphere. The raw materials