Wear Characteristics of Cone Crusher Lining Plates
Abstract The lining plates of cone crushers, as the most severely worn components, directly interact with ore materials, replacing critical parts such
Abstract The lining plates of cone crushers, as the most severely worn components, directly interact with ore materials, replacing critical parts such
The wear-resistant parts of sand casting crusher are still very common in China, such as jaw plate, high chromium plate
The research content comes from the school enterprise cooperation projects “research and development of new cone crusher liner” and “research
Three dimensional wear, also known as impact surface wear, mainly describes the wear mechanism on the three body impact abrasive
Two dimensional wear is also considered as surface wear. At this time, the wear mainly occurs on a two-dimensional plane,
Dimensional wear, also known as phase change wear, mainly describes the microstructure evolution and work hardening in the normal direction
Quenching process is an important part of the production process of iron and steel materials. The selection of quenching medium
The metallographic structure photo of the sample is given in Fig. 1. Under various process parameters, the experimental steel obtained
The normal temperature tension of the heat treated bainite Martian multiphase wear-resistant cast steel was carried out on the wdw-02a
According to the results of phase transformation point measurement, thermal expansion curve, metallographic structure observation and microhardness measurement, the self-designed
For the steel with determined composition, the relationship curve between transformation amount and time during the continuous cooling transformation of
JMatPro thermodynamic software is used to simulate the property diagram of the experimental steel under the designed composition system. The
The wear of crusher liner is mainly abrasive wear. Abrasive wear is a kind of wear caused by the migration
The experimental steel is smelted in the 25kg vacuum induction melting furnace (Fig. 1) of the Institute of engineering and
(1) Combined with the performance requirements and development direction of crusher liner materials and on the premise of less addition
The lining plate of cone crusher is a large casting. Combined with the requirements of industrial application, the performance requirements
The measured chemical composition of the experimental material is obtained by chemical analysis method and meets The measured chemical composition
In order to obtain the expected microstructure and properties of experimental steel, it is necessary to formulate appropriate heat treatment
Fracture, wear and corrosion are the three major failure forms of metal materials. For the abrasive wear condition of the
Taking experimental research as the starting point, gradually reveal the experimental law, put forward and improve the theory, and mainly
The moving cone liner (crushing wall) and the fixed cone liner (rolling mortar wall) are the main working parts and