Improving the Casting Process of Semi-Autogenous Mill Liner Casting
Abstract This paper discusses the improvement in the casting process of semi-autogenous mill liner casting. The existing casting process was
Abstract This paper discusses the improvement in the casting process of semi-autogenous mill liner casting. The existing casting process was
As the core component of the engine, the cylinder liner has put forward higher requirements for various performances of the
As shown in Figure 1: due to the impact of the grinding ball, the surface of the lining plate is
The following figure shows the stress field distribution of bimetal casting liner at different times during solidification. Due to the
According to the weight loss data of cast liner wear in the table, the relative wear coefficient of high chromium
The ball mill has been running for six months under full load and full working conditions. As shown in the
The following figure shows the temperature field distribution of the bimetal casting lining plate at different times during solidification. The
The installation test of high chromium cast iron carbon steel bimetallic liner was carried out on the wet ball mill
ANSYS is a general-purpose finite element software that can adapt to the coupling analysis of a variety of physical fields.
The control of the composite interface focuses on two aspects: one is to ensure the flatness of the composite interface,
For the liquid metal casting process, the interval between pouring of two metals is very critical: the interval is too
The high chromium cast iron carbon steel bimetallic casting lining plate was installed in the wet ball mill, and the
As shown in Figure 1, the left mold cavity is filled with high chromium cast iron liquid first, then flows
The composite thickness range of high chromium cast iron and carbon steel is shown in the figure below: According to
Using the vertical pouring process, it is necessary to insert an intermediate diaphragm at the junction of the two metals.
The chemical composition of high chromium cast iron in the test is shown in the table, and the analysis of
The traditional wear-resistant casting lining plate is generally made of high strength steel, low alloy steel and other materials by
(1) The dual liquid lost foam casting process is proposed to produce bimetallic liner. Placing the wear-resistant cast iron at
Thermoelastic and plastic models are used to calculate the thermal stress in the forming process of bimetal casting liner. The
In the process of lining plate forming, there are both heat absorption and cooling processes. During the heating process, the
Based on the finite element software, the temperature field, stress-strain field and their coupling in the casting process of carbon