Grey cast iron
Cast iron generally refers to a multi-component iron carbon alloy with a C content of more than 2.0% (wt%, the […]
Cast iron generally refers to a multi-component iron carbon alloy with a C content of more than 2.0% (wt%, the […]
Iron castings are widely used in various mechanical equipment, construction, metallurgy, agricultural machinery, national defense industry and other fields. In
The research object comes from the turbine rear exhaust pipe of ZHY casting. The turbine rear exhaust pipe is the
By controlling the size and distribution of graphite diameter and the spherical regularity of graphite, the correlation degree with the
ANSYS is a general-purpose finite element software that can adapt to the coupling analysis of a variety of physical fields.
The picture shows the microstructure of white cast iron in lost foam casting with and without vibration. It can be
The dual liquid bimetallic lining plate is a technology for preparing new composite wet wear resistant metal materials by using
The vibration lost foam casting technology is to apply a certain frequency and amplitude of mechanical vibration in the lost
The figure is the matrix structure diagram of the vibration lost foam casting ductile iron, in which figures (a) –
Fig. 1 (a) and Fig. 1 (b) show the hardness and strength changes of three groups of nodular cast iron
This paper mainly studies the effects of quenching temperature of destabilization treatment and natural aging treatment on the microstructure and
It can be seen from the discussion results that when the metal solidifies, the vibration will increase the undercooling of
The figure shows the relationship between Brinell hardness of gray cast iron and sample wall thickness. It can be seen
The metal melt meeting the thermodynamic conditions of nucleation only provides the possibility for the metal melt to solidify and
The figure shows the matrix structure of gray cast iron with different wall thickness. Among them, figures (a) and (a’),
The figure shows the relationship between the hardness of white cast iron and the wall thickness of the sample. It
The defects of traditional casting composite interface are avoided in principle. Solve the following problems: 1). Ordinary white cast iron,
The vibration solidification technology of lost foam casting is a physical modification technology to refine the grain size and improve
The figure shows the fracture morphology of grey cast iron prepared under different amplitude conditions. Among them, figures (a) –
Figure 1 shows the graphite morphology of the nodular cast iron by vibration lost foam casting, in which figure 1
The figure shows the matrix structure of gray prayer iron prepared under different vibration frequencies. Among them, figures (a) –
When the microcrack propagation no longer depends on the material surface conditions, the crack initiation stage ends, and the crack
The figure shows the austenite morphology of gray cast iron prepared under different vibration frequencies. Figures (a) – (d) show
Fig. 1 shows the microstructure SEM of three groups of ductile iron samples. It can be seen from the figure
The figure below shows the graphite morphology at different wall thicknesses of lost foam casting ductile iron. Figures (a) –
The effects of destabilizing heat treatment temperature and natural aging treatment on the microstructure and properties of high chromium cast
The figure shows the graphite morphology in gray cast iron with different wall thickness. Among them, figures (a) – (c)
It can be seen from the test that when the vibration frequency is 35Hz, the tensile strength of vibration lost
Under normal circumstances, the number of graphite balls in nodular cast iron will affect the matrix structure and stress distribution
The graphite in gray cast iron is flake, which is the most widely used cast iron, and its output accounts