Nodular cast iron plunger pump block
In the hydraulic system, the most important function similar to the “heart” is the high-pressure plunger pump, which is also […]
In the hydraulic system, the most important function similar to the “heart” is the high-pressure plunger pump, which is also […]
As a hydraulic component, plunger pump has the characteristics of precision, high cost and sensitivity to oil level pollution. When
As shown in the figure is the schematic diagram of the horizontal continuous casting cast iron profile production line. After
The figure shows the friction coefficient of different parts of lzqt600-3 ductile iron profile. The friction coefficients of the edge,
The production efficiency and yield of continuous casting billet can be improved by this process, the cost is lower than
The most important part of equipment manufacturing industry is hydraulic system, which plays an important role in various engineering fields.
With the development of computer hardware and simulation software and the maturity of various finite element software, the application of
Figure 1 shows SEM morphology of pearlite in different parts of lzqt600-3 ductile iron profile. The pearlite clusters in the
The design takes the tractor split axle housing as the research object. The axle housing is made of zg40mn low
The figure shows the matrix structure of lzqt600-3 ductile iron profile at different parts. In figure (a), the microstructure is
When the molten metal is poured into the mold, the volume shrinkage will occur during cooling and solidification. This shrinkage
The diameter distribution of graphite balls in three parts of lzqt600-3 ductile iron profile was analyzed by Excel and Image
The numerical simulation of temperature field is the basis of ProCAST software simulation, and also the core module. Through the
The shape factors of graphite balls in three parts of lzqt600-3 ductile iron profile were analyzed by Excel and Image
The figure shows the statistical results of the number of graphite balls in three parts of lzqt600-3 ductile iron profile.
In the filling process, the flow of molten metal will have a great impact on the quality of the axle
As shown in the figure is the structure diagram of polished state of lzqt600-3 ductile iron section edge, 1 /
ProCAST casting computer simulation process: firstly, Creo software was used to establish the three-dimensional numerical model of the casting system
The corrtest electrochemical test system can automatically carry out the electrochemical corrosion test and fit the test curve. Before the
The gating system is the channel to guide liquid metal into the mold cavity in sand mold. Its structure is
The friction and wear tests of nitrocarburizing samples were carried out on a friction and wear testing machine. The friction
Numerical simulation is a method that uses the correspondence between different things to verify measures. Numerical simulation is irreversible. Casting
Casting process parameters mainly include dimensional tolerance, linear shrinkage, draft angle and other aspects. The determination of these process parameters
According to the statistics of pearlite content in the structure of nodular cast iron under corrosion state, the gray data
In the molding process of sand coated iron mold, sand collapse and empty shell are the important reasons for sand
The linear shrinkage of the bridge shell has a great influence on the accuracy of the size of the bridge
Generally speaking, the higher the pouring temperature is, the better the fluidity of alloy liquid is, and the more favorable
Spheroidization rate is one of the important and often used evaluation criteria of ductile iron. The calculation method is as
For sand mold casting, in order to realize sand molding, mold taking, pouring riser setting and sand core installation, the
Based on the national standard GB / T 9441-2009 metallographic examination of nodular cast iron, the following four parameters are