Analysis on macro error sources of rapid investment casting
Because the sintered materials are mainly thermoplastic polymer materials and their composites, under the action of laser, the powder absorbs […]
Because the sintered materials are mainly thermoplastic polymer materials and their composites, under the action of laser, the powder absorbs […]
In SLS rapid investment casting process, there are SLS prototype preparation, SLS prototype post-processing and alloy casting solidification process, and
Since the emergence of centrifugal casting technology, many scholars at home and abroad have studied the centrifugal casting process. At
Based on the process of rapid investment casting, the source of dimension error in the process of rapid investment casting
(1) Taking the force of roller supported horizontal centrifugal casting machine as the research object, the calculation method of the
Selective laser sintering (SLS) is also known as selective laser sintering (SLS). As a processing technology based on the idea
(1) In horizontal centrifugal casting with roller support, the shape error and surface morphology of the two relative moving contact
The experimental and modeling studies on the heat transfer behavior and pressure transfer law of the casting die interface in
As the ball valve can be opened and closed only by turning the ball 1 / 4 circle, it belongs
The microstructure after heat treatment was observed and studied. It was found that there were various sizes of holes left
The displacement of casting is defined as the displacement of nodes caused by solidification shrinkage and punch pressing. As shown
Ball valve has the advantages of small flow resistance, quick opening and closing and easy pigging, which makes it widely
As shown in Figure 1, the pressure nephogram of aluminum alloy and magnesium alloy castings at different times (the pressure
The main functions and purposes of alloy heat treatment are as follows: one is to improve the process performance of
The driving device adopts direct push electro-hydraulic push rod. The speed of the electro-hydraulic push rod is fast, up to
The comprehensive mechanical properties of 7075 alloy wheel parts in as cast and T6 states by rheo squeeze casting were
Figure 1 (A-D) and figure 1 (E-G) show the solidification of aluminum and magnesium alloy castings at different times during
The inside of valve plate also needs pouring refractory layer, and the minimum width of valve plate is determined according
Although rheo squeeze casting can improve and improve the mechanical properties of 7075 alloy parts and eliminate some macro segregation,
As shown in the figure, the casting die interface pressure reaches the maximum value soon after the applied pressure. The
In order to isolate the high temperature of the pipeline, the high temperature resistant lining is poured inside the cylinder
In the solidification process of squeeze casting, on the one hand, due to the cooling of the casting, the metal
The simulation method based on ANSYS is used to solve the temperature field and stress field in squeeze casting process.
7075 aluminum alloy is a kind of high strength aluminum alloy which can be strengthened by heat treatment. High strength
(1) Based on the calculation module of AnyCasting, the material thermal property model and parameters of 7075 aluminum alloy wheel
In the process of casting, there are many factors that affect the heat transfer coefficient of the casting mold interface:
In the process of squeeze casting experiment, the material of the casting is aluminum alloy and magnesium alloy. The shape
The process of filling and solidification of 7075 aluminum alloy wheel parts in squeeze casting was simulated by AnyCasting software.
Denis et al. Systematically studied the interface heat transfer behavior between aluminum alloy and mold shell in investment casting process,
With the solidification process, the interface pressure gradually decreases to zero at some positions. When the interface pressure is reduced